General Information: This product is little flake has excellent heat stability and lubricity, with wide processing area. The lead compound stabilizer produced by our factory is simple to use and has no dust pollution, which can considerably reduce lead poisoning. Application: Mainly used in Pipe Fittings with excellent stability and lubricating property. Recommend dosage: 3.5-4.5 phr for PVC Pipe Fittings. Information provided by En-Door |