MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

CRP  Windform

Eastman Amphora™ AM3300 3D Polymer
Categories: Polymer; 3D Printing/Additive Manufacturing Polymer

Material Notes: Eastman Amphora™ AM3300 3D polymer is a low-odor, styrene-free material uniquely suited for 3D printing, particularly flexibility to print within a wide processing temperature range is needed. Amphora AM3300 has good flow properties through the printer nozzle—even at lower temperatures than some other polymers require. These properties make AM3300 more workable at a wider breadth of temperatures, producing reliable results and resulting in less waste. The model of functional aesthetics, Amphora AM3300 can be made into high-quality filament that exhibits advanced overhang ability, excellent looks, and large printing temperature range—empowering large panel of users to create durable and useful items. Amphora AM3300 is also a highly efficient polymer that can help speed up processing times. With the combination of a low processing temperature and an elevated temperature resistance, Amphora AM3300, can quickly print creations that are functional, durable, efficient, and attractive.

Application/Uses:

  • Production of 3D Printing filaments
Key Attributes:
  • Clarity and gloss
  • Dimensional stability
  • Enhanced aesthetics
  • Excellent toughness and temperature resistance
  • Extended Processing Window
  • FDA compliance
  • Low odor
  • Property retention in 3D applications
  • Styrene-free
  • Workability

Vendors:
Proto3000 provides design tools, 3D printers, additive manufacturing processes, metrology technologies, high-performance materials, and part-finishing automation. Our ISO 9001:2015 additive manufacturing production facility offers 3D printing services, rapid prototyping services, and end-part production with HP MultiJet Fusion (MJF), FDM, SLA, SLS, Polyjet, DLP, metal binder jetting, BMD, and DMLS.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.20 g/cc0.0434 lb/in³ASTM D792
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 105105ASTM D785
Tensile Strength at Break 35.0 MPa5080 psiASTM D638
Tensile Strength, Yield 50.0 MPa7250 psiASTM D638
Elongation at Break 193 %193 %ASTM D638
Elongation at Yield 4.5 %4.5 %ASTM D638
Flexural Strength 67.0 MPa9720 psiASTM D790
Flexural Modulus 1.80 GPa261 ksiASTM D790
Izod Impact, Notched  0.380 J/cm
@Temperature -40.0 °C
0.712 ft-lb/in
@Temperature -40.0 °F
ASTM D256
 0.700 J/cm
@Temperature 23.0 °C
1.31 ft-lb/in
@Temperature 73.4 °F
ASTM D256
Izod Impact, Unnotched  NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
ASTM D4812
 NB
@Temperature -40.0 °C
NB
@Temperature -40.0 °F
ASTM D4812
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 71.0 °C160 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 63.0 °C145 °FASTM D648
 
Processing PropertiesMetricEnglishComments
Melt Temperature 210 - 240 °C410 - 464 °F
 
Descriptive Properties
Processing - CoolingAs needed up to 100%
Processing - Heated Bed 60°C
Processing - InfillAs needed up to 100%
Processing - Layer Height0.1 or 0.2 mm
Processing - Minimal Layer Time4 s
Processing - Perimeterapprox. 1 mm
Processing - Speed30-100 mm/s

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Eastman Tritan™ TX2001 Copolyester
Eastman Tritan™ TX2000 Copolyester
Eastman Tritan™ LX201 Copolyester
Eastman Tritan™ FX100 Copolyester
Eastman DuraStar DS1000 Polymer, Natural

PE8930d / 217530

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.