Hostacom TRC 333N NA IVORY WHITE is a high flow thermoplastic olefinic elastomer (TPO) with excellent scratch resistance, very low stress whitening and low emissions and good stiffness/impact balance. It is typically used for interior trim applications. Status: Commercial - Restricted Availability: North America Application: Automotive Parts; Interior Automotive Applications Market: Automotive Processing Method: Injection Molding Attribute: Good Impact Resistance; Good Stiffness; Scratch Resistant Information provided by LyondellBasell. |