MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

SK Chemicals ECOZEN® Claro 100 Semi-crystalline Copolyester
Categories: Polymer; Thermoplastic; Polyester, TP; Polyethylene Terephthalate (PET)

Material Notes: ECOZEN® Claro is a semi-crystalline Copolyester grade, offering a combination of great clarity and chemical resistance. Articles manufactured with ECOZEN® Claro meet the definition of polyethylene terephthalate as ASTM-D7611-20 and the California Law's Public Resources Code Division 12.7 Plastic Waste Chapter 2. Containers and Packaging. Articles manufactured with ECOZEN® Claro are recyclable in the PET recycling stream. ECOZEN® Claro does not contain Bisphenol derivatives (BPA, etc.) and Phthalate-based plasticizer components regulated by the EU RoHS regulations. It also meets the requirements for food contact materials in Korea, the US, Europe, China, and Japan.

Applications: Cosmetic Packaging. Skin Care Packaging (Bottles, Jars). Consumer House wares. Attributes: Chemical Resistance. Clarity. Transparency.

Information provided by SK Chemicals

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.32 g/cc1.32 g/ccASTM D792
Linear Mold Shrinkage 0.0020 - 0.0050 cm/cm0.0020 - 0.0050 in/inASTM D955
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R >= 115>= 115ASTM D785
Tensile Strength at Break 43.1 MPa6250 psiASTM D638
Tensile Strength, Yield 59.8 MPa8670 psiASTM D638
Elongation at Break 200 %200 %ASTM D638
Elongation at Yield 5.0 %5.0 %ASTM D638
Flexural Strength 86.3 MPa12500 psiASTM D790
Flexural Modulus 2.45 GPa355 ksiASTM D790
Izod Impact, Notched 0.600 J/cm1.12 ft-lb/inASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 73.0 °C163 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 62.0 °C144 °FASTM D648
 
Optical PropertiesMetricEnglishComments
Haze <= 1.0 %<= 1.0 %ASTM D1003
UV Transmittance 89 %89 %ASTM D1003

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSK9937 / 291453

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.