MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Reliance Industries Relene E52009 Polyethylene
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Injection Molded

Material Notes: Relene E52009 is a High Density Polyethylene grade with low gel content, excellent orientation characteristics and negligible water carry-over. This grade is recommended for making raffia tapes and monofilaments with an excellent balance of high tenacity and good elongation.

Information provided by Reliance Industries

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.952 g/ccASTM D1505
Melt Flow 0.85 g/10 min
@Load 2.16 kg
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Film Tensile Strength at Yield, MD 34.5 MPaASTM D882
Film Tensile Strength at Yield, TD 37.5 MPaASTM D882
Film Elongation at Break, MD 900 %ASTM D882
Film Elongation at Break, TD 950 %ASTM D882
Elmendorf Tear Strength, MD 0.600 g/micronASTM D1922
Elmendorf Tear Strength, TD 1.70 g/micronASTM D1922
Dart Drop 1.50 g/micron38mm Dart, 66mm height; ASTM D1709
Film Tensile Strength at Break, MD 50.0 MPaASTM D882
Film Tensile Strength at Break, TD 45.0 MPaASTM D882

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Reliance Industries Reclair F18010 Polyethylene
Overview of materials for High Density Polyethylene (HDPE), Injection Molded
Reliance Industries Relene B31101 Polyethylene
Reliance Industries Relene B56003 Polyethylene
Reliance Industries Relene M60075 Polyethylene

PREL063 / 65403

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.