MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Lanxess Vocol® ZBPD-liq Rubber Processing Accelerator
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Function: Vocol ZBPD-liq is a fast curing secondary accelerator for NR and EPDM.

Composition: zinc dibutyldithiophosphate

Application: Molded and extruded technical rubber articles of all kinds, e.g. profiles, hoses, foils, coatings, and thick molded rubber components Vocol ZBPD-liq is regulated for use in articles in contact with food as specified under BgVV XXI, Category 4. Vocol ZBPD-liq is not regulated for use in FDA food contact applications.

Information provided by Lanxess.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.60 g/cc0.0578 lb/in³
 
Processing PropertiesMetricEnglishComments
Shelf Life 6.00 Month6.00 Month
 
Component Elements PropertiesMetricEnglishComments
Sulfur, S 22 - 23.6 %22 - 23.6 %ASTM D4927
 
Descriptive Properties
AppearanceAmber liquid

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PLANY9128 / 209519

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.