MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Primex Plastics Prime ABS Weather-X 500 Acrylonitrile Butadiene Styrene
Categories: Polymer; Thermoplastic; ABS Polymer; Acrylonitrile Butadiene Styrene (ABS), Extruded

Material Notes: Prime ABS Weather-X 500 is an ABS substrate with a co-extruded cap of an advanced Amorphous-Terpolymer of Acrylic-Styrene-Acrylonitrile. It offers exceptional durability in weather related environments without painting or other types of UV protection. It can retain its color stability under long-term exposure to the sun’s rays. It offers good aesthetics, color options, good chemical resistance and high heat performance.

Applications: This product is ideal for outdoor applications such as marine, ATV, RV, Spas, Pools and Lawn and Garden equipment or anywhere the above characteristics are required.

Information provided by Primex Plastics Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.05 g/ccASTM D792
Linear Mold Shrinkage 0.0030 - 0.0050 in/in
 0.0050 - 0.0080 in/inProcessing
Melt Flow 7.6 g/10 minASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 5640 psiASTM D638
Elongation, Ultimate 14.8 %ASTM D638
Flexural Modulus 322500 psiASTM D790
Izod Impact, Notched 3.70 ft-lb/in
@Temperature 0.000 °C
ASTM D256
 5.10 ft-lb/in
@Temperature 22.2 °C
ASTM D256
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) 210 °FAnnealed; ASTM D648
 
Processing PropertiesOriginal ValueComments
Processing Temperature 200 °FDe-mold
 220 - 300 °FPlug Temperature
 300 - 390 °FSurface Temperature
Mold Temperature 110 - 185 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PPRIM007 / 278478

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.