MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

SEKISUI SPI ALLEN® 8050TX PC/ABS Sheet
Categories: Polymer; Thermoplastic; ABS Polymer; Polycarbonate/ABS Alloy, Unreinforced

Material Notes: ALLEN® 8050TX is a general purpose PC/ABS with high impact strength and high heat deflection.

ALLEN® 8050TX meets Federal Motor Vehicle Safety Standard No. 302 (FMVSS302).

Suggested Application:

  • Vehicle Interior Trim
  • Covers and Housings
  • Fan Shrouds
  • Vehicle Exteriors (painted)
  • Instrument Panels
Features:
  • Custom color matching
  • Good forming properties
  • Edge trim easily used for future orders
  • High heat deflection temperature
  • High gloss finish
  • Meets many automotive specifications

Information provided by SEKISUI KYDEX, LLC.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.14 g/cc1.14 g/ccASTM D792
Water Absorption 0.170 %
@Time 86400 sec
0.170 %
@Time 24.0 hour
ASTM D570
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 117117ASTM D785
Tensile Strength 58.7 MPa8510 psiASTM D638
Tensile Modulus 2.468 GPa358.0 ksiASTM D638
Flexural Strength 94.5 MPa
@Strain 5.00 %
13700 psi
@Strain 5.00 %
ASTM D790
Flexural Modulus 2.58 GPa374 ksiASTM D790
Compressive Yield Strength 74.5 MPa10800 psiASTM D695
Bearing Yield Strength <= 248.9 MPa<= 36100 psiASTM D953
 26.3 MPa
@Strain 4.00 %
3810 psi
@Strain 4.00 %
ASTM D953
Shear Strength 61.1 MPa8860 psiASTM D732
Izod Impact, Notched 4.378 J/cm8.202 ft-lb/inASTM D256
 5.552 J/cm10.40 ft-lb/inASTM D256
Gardner Impact 71.4 J52.7 ft-lbDrop Dart Impact, GE; ASTM D5420
 
Electrical PropertiesMetricEnglishComments
Dielectric Strength 18.9 kV/mm480 kV/inoil; ASTM D149
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 65.6 µm/m-°C36.4 µin/in-°FASTM E831
Deflection Temperature at 0.46 MPa (66 psi) 130 °C266 °Fannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 122 °C252 °Fannealed; ASTM D648

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSEKIS527 / 325267

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.