AFFINITY™ EG 8100G Polyolefin Plastomer (POP) is produced via INSITE™ Technology. It is a general purpose ethylene-octene copolymer exhibiting high flexibility and elasticity. It can be utilized in monolayer and coextruded films and in blends with other polyolefins to enhance clarity, sealability and toughness of the structure. Information provided by Dow |