MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Morgan Advanced Ceramics Z-Blok 3 Modules Cerachrome Blanket
Categories: Ceramic; Oxide

Material Notes: Z-Blok 3 side-fix modules are convoluted blanket modules which combine the excellent thermal characteristics and proven service performance of Thermal Ceramics’ Z-Bloks with the ease of installation and versatility of the T-Bar anchoring system. They are made from high quality spun-fibre Blanket, folded and pre-compressed to a specified density, and held in position with 2 stainless steel tubes, mounted transversely within the module. The modules can be supplied encapsulated in plastic film, which ensures dust levels are kept to a minimum during installation. During installation, the modules are further compressed, the resilience of the fiber and recovery after the restraining bands are removed ensuring tightly-compressed intermodular joints.

Typical Applications: Z-Blok 3 has a multitude of uses in heat containment applications in all industry groups, some of which are: *Petrochemical: Process heaters, reformers, ductwork and pyrolysis heaters. *Iron and Steel: Transfer ladle lids, soaking pit covers, reheating furnace, multi and single stack coil annealing furnaces, continuous annealing and coating furnaces, rotary hearth furnaces, car bottom furnaces, roller furnaces, lift-off furnaces, offtakes and ductwork. *Aluminium: Soaking pits and covers, bale out furnaces, homogenizing furnaces and ductwork. *Ceramic:Tunnel kilns for whiteware and red brick, intermittent kilns for whiteware and red brick, Hoffman Kilns and ductwork. *Utilities: Thermal oxidizers, waste heat recovery units, combustion chambers and boiler ductwork.

Information provided by Morgan Advanced Materials

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.128 - 0.160 g/cc
 
Thermal PropertiesOriginal ValueComments
Specific Heat Capacity 1.13 J/g-°C
@Temperature 1090 °C
Thermal Conductivity 0.110 W/m-K
@Temperature 400 °C
at 160 kg/m3
 0.120 W/m-K
@Temperature 400 °C
at 128 kg/m3
 0.160 W/m-K
@Temperature 600 °C
at 160 kg/m3
 0.190 W/m-K
@Temperature 600 °C
at 128 kg/m3
 0.230 W/m-K
@Temperature 800 °C
at 160 kg/m3
 0.270 W/m-K
@Temperature 800 °C
at 128 kg/m3
 0.310 W/m-K
@Temperature 1000 °C
at 160 kg/m3
 0.360 W/m-K
@Temperature 1000 °C
at 128 kg/m3
 
Descriptive Properties
Classification Temperature (°C)1425
Colorblue/green

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

CMORF7098 / 203396

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.