MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Melos Mecoline S TP 1006 F CHAR Halogen-free, thermoplastic, flame retardant sheathing
Categories: Polymer; Thermoplastic

Material Notes: Halogen-free, thermoplastic, highly flame retardant sheathing compound for low and medium voltage cables

Compound class: Sheathing

Compound category: TP

Flame retardant: ATH

Standards: VDE 0207 part 24 HM 2; VDE 0250 part 215 HM 5; IEC 60092-360 SHF 1

Typical applications: Halogen-free, low smoke, thermoplastic, highly flame retardant char formation compound for the sheathing of low and medium voltage cables in General Installation applications.

Features: Flame retardant; Halogen-free; Low smoke

Information provided by Melos

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.55 g/cc0.0560 lb/in³pressed plaques, 155°C / 5 min; DIN EN ISO 1183-1A
pH >= 4.5>= 4.5Corrosivity, Acid gas emission; IEC 60754-2
Melt Flow 3.2 g/10 min
@Load 21.6 kg,
Temperature 160 °C
3.2 g/10 min
@Load 47.6 lb,
Temperature 320 °F
DIN EN ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 4747pressed plaques, 155°C / 5 min; DIN ISO 7619-1
Tensile Strength 9.20 MPa1330 psiextruded tapes; IEC 60811-501
 10.304 MPa
@Temperature 100 °C,
Time 1.21e+6 sec
1494.5 psi
@Temperature 212 °F,
Time 336 hour
extruded tapes, After ageing in air oven; IEC 60811-401
 10.5 MPa
@Temperature 100 °C,
Time 605000 sec
1520 psi
@Temperature 212 °F,
Time 168 hour
extruded tapes, After ageing in air oven; IEC 60811-401
Elongation at Break 195 %195 %extruded tapes; IEC 60811-501
 146.055 %
@Temperature 100 °C,
Time 605000 sec
146.055 %
@Temperature 212 °F,
Time 168 hour
extruded tapes, After ageing in air oven; IEC 60811-401
 157.95 %
@Temperature 100 °C,
Time 1.21e+6 sec
157.95 %
@Temperature 212 °F,
Time 336 hour
extruded tapes, After ageing in air oven; IEC 60811-401
Penetration 40
@Temperature 80.0 °C,
Time 21600 sec
40
@Temperature 176 °F,
Time 6.00 hour
[%] Hot pressure test, extruded tapes; IEC 60811-508
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 5.60e+11 ohm-cm5.60e+11 ohm-cm500V; DIN IEC 60093
Dielectric Strength 27.6 kV/mm701 kV/inIEC 60243-1
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 80.0 °C176 °F
Minimum Service Temperature, Air -25.0 °C-13.0 °F
Flammability, UL94  V-0
@Thickness 2.00 mm
V-0
@Thickness 0.0787 in
Vertical
 V-0
@Thickness 3.00 mm
V-0
@Thickness 0.118 in
Vertical
 
Processing PropertiesMetricEnglishComments
Processing Temperature 150 - 170 °C302 - 338 °FTool
 155 - 165 °C311 - 329 °FMaximum mass temperature
Zone 1 110 - 130 °C230 - 266 °F
Zone 2 115 - 135 °C239 - 275 °F
Zone 3 120 - 140 °C248 - 284 °F
Zone 4 125 - 145 °C257 - 293 °F
Zone 5 130 - 150 °C266 - 302 °F
Adapter Temperature 135 - 155 °C275 - 311 °F
Head Temperature 140 - 160 °C284 - 320 °F
Drying Temperature 60.0 - 70.0 °C140 - 158 °F
Dry Time 4.00 - 6.00 hour4.00 - 6.00 hour
Shelf Life 12.0 Month12.0 Month
 
Component Elements PropertiesMetricEnglishComments
Loss on Ignition(%) 41 %41 %pressed plaques, 155°C / 5 min.; ASTM D 2863 A
 
Descriptive Properties
Conductivity=10 µS/mmpressed plaques, 155°C / 5 min, IEC 60754-2
Temperature index290°Cpressed plaques, ASTM D 2863 D

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PMELOS005 / 296112

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.