Kobe Steel KSTI-1.5AL Alpha Titanium Alloy, Annealed
Categories:
Metal
;
Nonferrous Metal
;
Titanium Alloy
Material Notes:
Nominal Composition: Ti-1.5 Al
Applications:
Exhaust systems.
Features:
Heat resistant.
Information provided by Kobe Steel
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Mechanical Properties
Metric
English
Comments
Tensile Strength, Ultimate
>=
345
MPa
>=
50000
psi
Tensile Strength, Yield
215
-
450
MPa
31200
-
65300
psi
0.2% proof
Elongation at Break
>= 20 %
>= 20 %
Reduction of Area
>= 30 %
>= 30 %
Bend Radius, Minimum
2.0
t
2.0
t
t ≤ 1.8 mm
2.5
t
2.5
t
1.8 < t ≤ 4.75 mm
Component Elements Properties
Metric
English
Comments
Aluminum, Al
1.0 - 2.0 %
1.0 - 2.0 %
Carbon, C
<= 0.080 %
<= 0.080 %
Hydrogen, H
<= 0.015 %
<= 0.015 %
Iron, Fe
<= 0.30 %
<= 0.30 %
Nitrogen, N
<= 0.030 %
<= 0.030 %
Oxygen, O
<= 0.25 %
<= 0.25 %
Titanium, Ti
>= 97.325 %
>= 97.325 %
As Remainder
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
Users viewing this material also viewed the following:
Kobe Steel KS6-2-4-2 Alpha Titanium Alloy, AMS 4976, Solution treated and aged
ATI Allegheny Ludlum Grade 2 Titanium (UNS R50400)
ATI Allegheny Ludlum Grade 1 Titanium (UNS R50250)
Kobe Steel KS-6-2-4-6 Alpha-Beta Titanium Alloy, AMS 4981, Solution treated and aged. Thickness ≤ 3 in.
Kobe Steel KS60AKOT Titanium alloy with low alloying elements, ASTM Gr. 33, Annealed
NKOBE11 / 17758
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.