MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

3M 7260M High Temperature Over Spray Protective Bags and Sheets
Categories: Polymer; Adhesive

Material Notes: 3M™ High Temperature Over Spray Protective Bags and Sheets 7260M are used for masking where high temperature resistance or custom sizes are needed. This high performance product is designed for masking cars and light trucks during OEM painting, and for industrial paint masking applications such as truck, bus, RV, heavy equipment, and aircraft.

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Thickness 41.1 microns1.62 milWeight based; ASTM E252
 45.7 microns1.80 milCaliper; ASTM D374
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 19.3 MPa2790 psiMachine Direction; ASTM D3756
 21.4 MPa3110 psiCross Direction; ASTM D3756
Elongation at Break 700 %700 %ASTM D3756
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 315 °C599 °Ffor 1 hr
 
Processing PropertiesMetricEnglishComments
Shelf Life 12.0 Month12.0 Month
 
Descriptive Properties
AppearanceTranslucent

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Resinlab® RC8060 Anaerobic Retaining Compound
Cookson Group STAYSTIK® 882 Alumina Filled "Low Flow" Dielectric Film

PMM33982 / 168729

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.