MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
BASF ecovio® IS1335 PLA
Categories: Polymer; Thermoplastic; Polylactic Acid (PLA) Biopolymer

Material Notes: Product Description: Mineral filled injection molding grade, bio-degradable according to DIN EN 13432, e/g/ for stiff packaging applications in food contact. BASF ecovio® IS (Injection Specialty) grade are plastics for articles intended to come onto contact with foodstuffs. These plastics fulfill different food regulatory norms like e.g. FDA, European Food Contact n°2002/72/EC and/or GMP (EC) n°2023/2006.

Availability: Europe; North America

Filler/Reinforcement: Mineral, 30% Filler by Weight

Features: Biodegradable; Compostable; Food Contact Acceptable

Use: Food Packaging

Agency Ratings: ASTM D6400; DIN EN 13432; EC 1907/2006 (REACH); EC 2023/2006; EU 2002/72/EC; FDA FCN 178: FDA FCN 475; FDA FCN 907; FDA Food Contact

RoSH Compliance: RoSH Compliant

Form: Pellets

Processing Method: Injection Molding

Information provided by BASF Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.47 g/ccISO 1183
Maximum Moisture Content 0.080
Linear Mold Shrinkage 0.0014 cm/cm
@Thickness 1.00 mm
ISO 294-4
Linear Mold Shrinkage, Flow 0.0010 cm/cmISO 294-4
Linear Mold Shrinkage, Transverse 0.0020 cm/cmISO 294-4
Melt Flow 9.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Elongation at Break 4.0 %ISO 527-2/50
Tensile Modulus 522000 psiISO 527-1
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 131 °FISO 75-2/B
 
Processing PropertiesOriginal ValueComments
Processing Temperature 77.0 °FHopper
Rear Barrel Temperature 356 °F
Middle Barrel Temperature 365 °F
Front Barrel Temperature 374 °F
Nozzle Temperature 383 °F
Melt Temperature 356 - 401 °F
Mold Temperature 50.0 - 104 °F
Drying Temperature 176 °F
Dry Time 5.00 hour

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PBASG2154 / 310847

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.