MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

HB Fuller 173 Adhesive
Categories: Polymer; Thermoplastic; Adhesives, Sealants, and Coatings

Material Notes: 173 is a hydraulic sealant, general purpose, fittings up to ¾ inch diameter. Ideal for fine threads, 173 is a low viscosity, medium strength thread and pipe sealant.

Features and Benefits:

  • High Pressure Fluid Sealant
  • Stable in Harsh Environments
  • Excellent Chemical Resistance
  • Excellent Vibration Resistance
  • Low Viscosity for Improved Flow and Coverage

Information provided by H.B. Fuller Company

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.06 g/cc1.06 g/cc
Viscosity 500 cP500 cP
 
Mechanical PropertiesMetricEnglishComments
Shear Strength 8.00 - 12.0 MPa1160 - 1740 psiPin/Collar; ISO 10123
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 150 °C302 °F
Minimum Service Temperature, Air -55.0 °C-67.0 °F
Flash Point >= 100 °C>= 212 °F
 
Processing PropertiesMetricEnglishComments
Cure Time 10.0 - 20.0 min0.167 - 0.333 hourHandling Strength
 60.0 - 180 min1.00 - 3.00 hourFunctional Strength
 300 - 600 min5.00 - 10.0 hourFull
 
Descriptive Properties
ColorBrown
ConsistencyLiquid
Torque12-16 in-lbBreakaway, ISO 10964
 18-24 in-lbPrevailing, ISO 10964

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PHBFULL127 / 316918

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.