MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Poly Alloy XuanWu™ XW3110 PP, Impact Grade
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Impact Modified; Molded/Extruded

Material Notes: XuanWu XW 3110 resin is a mechanical reinforcement polyethylene compound which has excellent impact property, especially under low temperature. XW3110 also has perfect performance on chemical resistance and anti wearing

Information provided by Poly Alloy Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.955 g/cc0.955 g/ccASTM D792
Melt Flow 4.0 g/10 min
@Load 5.00 kg,
Temperature 230 °C
4.0 g/10 min
@Load 11.0 lb,
Temperature 446 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 24.5 MPa3560 psiASTM D638
Elongation at Break >= 300 %>= 300 %ASTM D638
Flexural Strength 29.4 MPa4270 psiASTM D790
Flexural Modulus 0.981 GPa142 ksiASTM D790
Izod Impact, Notched  NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
ASTM D256
 NB
@Temperature -30.0 °C
NB
@Temperature -22.0 °F
ASTM D256
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 210 - 220 °C410 - 428 °F
Middle Barrel Temperature 220 - 230 °C428 - 446 °F
Front Barrel Temperature 220 - 230 °C428 - 446 °F
Nozzle Temperature 220 - 230 °C428 - 446 °F
Mold Temperature 40.0 - 50.0 °C104 - 122 °F
Drying Temperature 80.0 °C176 °F
Dry Time 2.00 hour2.00 hour
Shelf Life 24.0 Month24.0 Month

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PPALLOY083 / 278362

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.