MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Röchling SUSTAPEEK® GLD 140 FG natural PEEK
Categories: Polymer; Thermoplastic; Polyketone; Polyetheretherketone (PEEK); Polyetheretherketone, PEEK, Unreinforced

Material Notes: Product characteristics:
  • Excellent dimensional stability
  • Very good sliding behavior
  • Suitable for contact with foodstuffs according to (EC) No. 1935/2004
Product applications:
  • Food processing industry

Information provided by Röchling.

Vendors: Ensinger TECAPEEK™ shapes are manufactured exclusively with Victrex™ PEEK polymer. The Ensinger process and Victrex resins ensure reliability, consistency, dimensional stability, and high temperature mechanical performance.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.36 g/cc0.0491 lb/in³DIN EN ISO 1183-1
Water Absorption 0.20 %0.20 %DIN EN ISO 62
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 8686DIN EN ISO 868
Tensile Strength, Yield 87.0 MPa12600 psiDIN EN ISO 527
Elongation at Break 3.0 %3.0 %DIN EN ISO 527
Modulus of Elasticity 3.70 GPa537 ksiDIN EN ISO 527
Izod Impact, Notched (ISO) 3.50 kJ/m²1.67 ft-lb/in²DIN EN ISO 179
 
Electrical PropertiesMetricEnglishComments
Surface Resistance 1.00e+16 ohm1.00e+16 ohmDIN EN 62631-3-2
Dielectric Strength 20.0 kV/mm508 kV/inIEC 60243
 
Thermal PropertiesMetricEnglishComments
CTE, linear 55.0 µm/m-°C30.6 µin/in-°FDIN 53752
Melting Point 343 °C649 °FISO 11357-3
Maximum Service Temperature, Air 250 °C482 °Flong term
 310 °C590 °Fshort term
Minimum Service Temperature, Air -30.0 °C-22.0 °F
Flammability, UL94  V-0
@Thickness 3.00 mm
V-0
@Thickness 0.118 in
 V-0
@Thickness 6.00 mm
V-0
@Thickness 0.236 in
 
Compliance PropertiesMetricEnglishComments
European Food 1935/2004 YesYes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Röchling SUSTAPEEK® PEEK
Röchling SUSTAPEEK® PEEK
Röchling SUSTAPEEK® MOD ESD 90
Röchling SUSTAPEEK® MOD
Röchling SUSTAPEEK® MG natural Medical Grade PEEK

PROCH9323 / 233025

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.