MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Morgan Advanced Ceramics Kaowool™ VF Shapes 1260 Thermal Ceramic
Categories: Ceramic; Oxide

Material Notes: Kaowool TM VF Shapes are insulating products made from a mixture of refractory ceramic fiber by vacuum forming. This process allows the production of a variety of configurations, tailored to the particular application and ranging from simple sections (such as sleeves, cones) to complex shapes. compositions are available for service temperatures from 1260°C to 1600°C. Shapes can also be produced in a strong composition which gives higher strength and density. Thermal properties are similar to the normal grades but with improved resistance to erosion. These versatile products can be used where rigid shapes, self supporting are required for high temperature insulation (according to the mix). Designed as per customer drawings, they are easy to install.

Information provided by Morgan Advanced Materials

Key Words: Thermal Ceramics
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.280 g/cc0.0101 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Modulus of Rupture <= 0.00140 GPa<= 0.203 ksi
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity  0.0700 W/m-K
@Temperature 200 °C
0.486 BTU-in/hr-ft²-°F
@Temperature 392 °F
ASTM C-201
 0.0900 W/m-K
@Temperature 400 °C
0.625 BTU-in/hr-ft²-°F
@Temperature 752 °F
ASTM C-201
 0.110 W/m-K
@Temperature 600 °C
0.763 BTU-in/hr-ft²-°F
@Temperature 1110 °F
ASTM C-201
 0.150 W/m-K
@Temperature 800 °C
1.04 BTU-in/hr-ft²-°F
@Temperature 1470 °F
ASTM C-201
Maximum Service Temperature, Air 1600 °C2910 °F
 
Descriptive Properties
Approx. weight loss on 1st firing (%)5-7
Classification Temperature (°C)1260
Colorwhite/tan

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

CMORF6216 / 203000

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.