MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Beologic Beograde THF040 Extrusion
Categories: Polymer; Thermoplastic

Material Notes: Main properties: biodegradable, high stiffness. Applications: film, thermoforming, indoor, outdoor, food applications

Information provided by Beologic.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.25 - 1.35 g/cc0.0452 - 0.0488 lb/in³ISO 1183-1
Melt Flow 2.0 - 3.0 g/10 min
@Load 2.16 kg,
Temperature 90.0 °C
2.0 - 3.0 g/10 min
@Load 4.76 lb,
Temperature 194 °F
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 20.9 MPa3030 psiISO 527-1
Tensile Strength 40.0 MPa5800 psiISO 527-1
Elongation at Break 5.0 %5.0 %ISO 527-1
Tensile Modulus 3.52 GPa511 ksiISO 527-1
Flexural Modulus 3.092 GPa448.5 ksiISO 178
Charpy Impact, Notched 0.990 J/cm²4.71 ft-lb/in²ISO 179-1eA
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 57.8 °C136 °FISO 75-1 (B)
 
Descriptive Properties
Beologic Article Number9802070040
BiodegradableyesEN13432
Carbon footprint (kg CO2 eq/kg)3.514PAS 2050
Renewable contentyes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PBEOL9831 / 314117

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.