MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Shandong Dongyue Polymer DF-201 PTFE Fine Powder
Categories: Polymer; Thermoplastic; Fluoropolymer; Polytetrafluoroethylene (PTFE); PTFE Powder

Material Notes: Usage: It is suitable for making unsintered tape.

Packing: PTFE is packed in double layer PVC bags inside and in hard circular barrels outside.

Storage: PTFE should be stored in a clean, dry warehouse to protect from dust, moisture, etc.

Transportation: The products are transported according to non-dangerous products. Heat, moisture, freezing and strong shock should be avoided during transportation. Over-bumpiness and compression is apt to make the resin bind together.

Conformable with Q/DYG 004-2003

Information provided by Shandong Dongyue Polymer Material Co., Ltd

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 2.20 g/cc
Bulk Density 0.375 - 0.575 g/cc
Particle Size 375 - 675 µm
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength >= 18.6 MPaQualified
 >= 20.7 MPaGrade A
 >= 24.0 MPaExcellent
Elongation at Break >= 350 %
 
Electrical PropertiesOriginal ValueComments
Dielectric Strength <= 2.10 kV/mm
Dissipation Factor 0.00030
 
Thermal PropertiesOriginal ValueComments
Melting Point 322 - 332 °C
 
Processing PropertiesOriginal ValueComments
Moisture Content <= 0.040 %
 
Descriptive Properties
Extrude Pressure (MPa)5.5-13.9RR100
For CheckExecute according to requirement of HG/T3028-1999
For ProcessPaste Extrusion
Smoothness & CleanlinessExcellent: White sheet surface, fiber is average, no gravel and metallic powder, even sheet texture < 1 for mechanical impurity (>0.5mm) or organic impurity (>2mm)
 Grade A: White sheet surface, fiber is average, no gravel and metallic powder, even sheet texture < 1 for mechanical impurity (>0.5mm) or organic impurity (>2mm)
 Qualified: White sheet surface, fiber is average, no gravel and metallic powder, allow 0.5mm organic impurity
Thermal Inst. Index<50

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Shandong Dongyue Polymer DF-202 PTFE Fine Powder
Shandong Dongyue Polymer DF-17 PTFE Molding Powder (Micronized Particles)
Shandong Dongyue Polymer DF-16 PTFE Molding Powder (Micronized Particles)
Shandong Dongyue Polymer DF-11 PTFE Molding Powder (Micronized Particles)
Shandong Dongyue Polymer DF-203 PTFE Fine Powder

PSHADP05 / 103656

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.