MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Wolf Kunststoff INKUFLON P F1A
Categories: Polymer; Thermoplastic

Material Notes:

Information provided by Wolf Kunststoff

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 2.14 - 2.18 g/cc0.0773 - 0.0788 lb/in³ISO 1183
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 51 - 6051 - 60DIN 53505
Ball Indentation Hardness 22.0 - 32.0 MPa3190 - 4640 psiH358/30; DIN 2039
Tensile Strength 20.0 - 30.0 MPa2900 - 4350 psiDIN EN ISO 527
Elongation at Break 250 - 400 %250 - 400 %DIN EN ISO 527
Compressive Strength 8.00 MPa1160 psiat 3,5% strain; DIN EN ISO 604
Coefficient of Friction, Dynamic 0.060
@Temperature 20.0 °C
0.060
@Temperature 68.0 °F
Limiting Pressure Velocity 0.00330 MPa-m/sec94.2 psi-ft/minv=100m/min
 0.00830 MPa-m/sec237 psi-ft/minv=1m/min
 0.00830 MPa-m/sec237 psi-ft/minv=10m/min
 
Electrical PropertiesMetricEnglishComments
Dissipation Factor <= 0.00030
@Frequency 110 Hz
<= 0.00030
@Frequency 110 Hz
IEC 112
 
Thermal PropertiesMetricEnglishComments
CTE, linear 122 µm/m-°C
@Temperature 100 °C
67.8 µin/in-°F
@Temperature 212 °F
ISO E 830
Thermal Conductivity 0.230 W/m-K1.60 BTU-in/hr-ft²-°FDIN 52612
 
Descriptive Properties
ColorWhite
Free from PTFENot applicable
Machined partsApplicable
Resistance to chemicals10Nominal Scale: 1, low; 10, high
Rods up to øe (de)Applicable
Sheets up to max. thicknessApplicable

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PZEDEX3008 / 250065

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.