MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Borealis Bormod™ HC904CF Polypropylene  (discontinued **)
Categories: Polymer; Thermoplastic; Polypropylene (PP)

Material Notes: Bormod™ BJ368MO is a polypropylene copolymer characterized by good flow, and optimum combination of high stiffness and high impact strength. The material is nucleated with Borstar® Nucleation Technology (BNT). Flow properties, nucleation and good stiffness give potential for cycle time reduction. The material have good antistatic performance and good mould release properties. Applications: Thin wall containers.

Information provided by Borealis AG

Key Words: PP
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.905 g/cc0.0327 lb/in³ISO 1183
Melt Flow 2.8 g/10 min
@Load 2.16 kg,
Temperature 230 °C
2.8 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 39.5 MPa5730 psi50mm/min; ISO 527-2
Film Elongation at Break, MD 158 %158 %blown films; ISO 527-3
 450 %450 %cast films; ISO 527-3
Film Elongation at Break, TD 4.0 %4.0 %blown films; ISO 527-3
 5.0 %5.0 %cast films; ISO 527-3
Elongation at Yield 7.0 %7.0 %ISO 527-2
Tensile Modulus 1.55 GPa225 ksiroll stack films TD; ISO 527-3
 1.70 GPa247 ksiroll stack films MD; ISO 527-3
 1.70 GPa247 ksicast films TD; ISO 527-3
 1.875 GPa271.9 ksicast films MD; ISO 527-3
 2.05 GPa297 ksiblown films MD; ISO 527-3
 2.07 GPa300 ksiblown films TD; ISO 527-3
Flexural Modulus 2.00 GPa290 ksi50% humidity; ISO 178
Charpy Impact, Notched 0.400 J/cm²
@Temperature 23.0 °C
1.90 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eA
Dart Drop, Total Energy  1.00 J
@Thickness 0.0500 mm
0.738 ft-lb
@Thickness 0.00197 in
cast films; ISO 7765-2
 1.00 J
@Thickness 0.300 mm
0.738 ft-lb
@Thickness 0.0118 in
roll stack films; ISO 7765-2
Coefficient of Friction 0.30 - 0.400.30 - 0.40film to film; cast; ISO 8295
 0.30 - 0.400.30 - 0.40film to film;blown; ISO 8295
Dart Drop Test >= 25.0 g
@Thickness 0.0500 mm
>= 0.0551 lb
@Thickness 0.00197 in
blown films; ISO 7765-1
Film Tensile Strength at Break, MD 42.0 MPa6090 psiblown films; ISO 527-3
 60.0 MPa8700 psicast films; ISO 527-3
Film Tensile Strength at Break, TD 40.0 MPa5800 psicast films; ISO 527-3
 42.0 MPa6090 psiblown films; ISO 527-3
 
Thermal PropertiesMetricEnglishComments
Melting Point 166 °C331 °FDSC; ISO 3146
Deflection Temperature at 0.46 MPa (66 psi) 118 °C244 °FISO 75-2
Vicat Softening Point 156 °C
@Load 1.02 kg
313 °F
@Load 2.25 lb
A50; ISO 306
 
Optical PropertiesMetricEnglishComments
Haze <= 5.0 %<= 5.0 %Cast Film; ASTM D1003
 <= 13.5 %<= 13.5 %roll stack films; ASTM D1003
 <= 14 %<= 14 %blown films; ASTM D1003
Gloss >= 45 %>= 45 %20° of arc, blown films; ASTM D2457
 >= 110 %>= 110 %20° of arc, cast films; ASTM D2457
 >= 130 %>= 130 %20° of arc, roll stack films; ASTM D2457

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Total PPC 1645 Polypropylene, Heterophasic Copolymer, Pipes
Braskem H 502HC Thermoforming Polypropylene Homopolymer
Overview of materials for Polypropylene, Molded
Borealis RA7050-GN Polypropylene-Random-Copolymer for Pressure Pipe Systems
Borealis RA7050 Polypropylene-Random-Copolymer for Pressure Pipe Systems

PBOREA379 / 108638

Elmet Technologies

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.