MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Coosa Composites Nautical 20 12 mm Fiberglass Reinforced Polyurethane Foam Panel
Categories: Polymer; Thermoset; Polyurethane, TS; Thermoset Polyurethane Foam, Glass Filled

Material Notes: The Nautical product is Coosa’s lightest fiberglass reinforced composite panel and an excellent replacement for plywood and other wood core composite panels due to its high strength to low weight ratio.

Nautical 20 Composite Panel: Nautical 20 is Coosa’s economical alternative in the Nautical series and the perfect middle ground between Nautical 24 and Nautical 15. With a density of 20 pounds per cubic foot, it is 45% or more lighter than plywood, providing versatility for various applications.

Information provided by Coosa Composites

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 20.0 lb/ft³ASTM C271
Thickness 12000 microns
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 4.10 MPaFlatwise; ASTM C297
Flexural Strength 18.6 MPaASTM D790
Flexural Modulus 632 MPaASTM D790
Compressive Strength 4.10 MPaCore; ASTM C365
Compressive Modulus 92.0 MPaCore; ASTM C365
Shear Modulus 0.0205 GPaCore; ASTM C273
Shear Strength 3.10 MPaCore; ASTM C273

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PCOOS908 / 322928

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.