MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Sandvik SAF 2205 Plate, Sheet and Coil
Categories: Metal; Ferrous Metal; Duplex; Stainless Steel

Material Notes: Sandvik SANMAC SAF 2205™ is a duplex stainless steel (austenitic-ferritic). It is characterized by:
  • high resistance to stress corrosion cracking in chloride-bearing environments
  • high resistance to stress corrosion cracking in environments containing hydrogen sulphide
  • high resistance to general corrosion, pitting and crevice corrosion
  • high mechanical strength – roughly twice the proof strength of austenitic stainless steels excellent machinability
  • good hot-working properties
  • high resistance to erosion corrosion and corrosion fatigue
  • physical properties that offer design advantages
  • good weldability
  • Information provided by Sandvik

    UNS S31803, S32205; EN 1.4462

    Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
     
    Physical PropertiesOriginal ValueComments
    Density 7.80 g/cc
     
    Mechanical PropertiesOriginal ValueComments
    Hardness, Brinell <= 290
    Tensile Strength, Ultimate >= 620 MPa20 mm wall thickness
     >= 560 MPa
    @Temperature 300 °C
     >= 630 MPa
    @Temperature 100 °C
    Tensile Strength, Yield >= 450 MPa
    @Strain 0.2 %
    20 mm wall thickness
     >= 500 MPa
    @Strain 1 %
    20 mm wall thickness
     >= 310 MPa
    @Strain 0.2 %,
    Temperature 300 °C
     320 MPa
    @Strain 0.2 %,
    Temperature 250 °C
     330 MPa
    @Strain 0.2 %,
    Temperature 200 °C
     >= 340 MPa
    @Strain 1 %,
    Temperature 300 °C
     345 MPa
    @Strain 0.2 %,
    Temperature 150 °C
     350 MPa
    @Strain 1 %,
    Temperature 250 °C
     360 MPa
    @Strain 1 %,
    Temperature 200 °C
     >= 370 MPa
    @Strain 0.2 %,
    Temperature 100 °C
     385 MPa
    @Strain 1 %,
    Temperature 150 °C
     >= 420 MPa
    @Strain 1 %,
    Temperature 100 °C
    Elongation at Break >= 25 %2", 20 mm wall thickness
     >= 25 %20 mm wall thickness
    Modulus of Elasticity 200 GPa
     180 GPa
    @Temperature 300 °C
     186 GPa
    @Temperature 200 °C
     194 GPa
    @Temperature 100 °C
    Charpy Impact 50.0 J
    @Temperature -100 °C
     162 J
    @Temperature -50.0 °C
     250 J
    @Temperature 0.000 °C
     
    Thermal PropertiesOriginal ValueComments
    CTE, linear 13.0 µm/m-°C
    @Temperature 30.0 - 100 °C
     13.5 µm/m-°C
    @Temperature 30.0 - 200 °C
     14.0 µm/m-°C
    @Temperature 30.0 - 300 °C
     14.5 µm/m-°C
    @Temperature 30.0 - 400 °C
    Specific Heat Capacity 0.480 J/g-°C
    @Temperature 20.0 °C
     0.500 J/g-°C
    @Temperature 100 °C
     0.530 J/g-°C
    @Temperature 200 °C
     0.550 J/g-°C
    @Temperature 300 °C
     0.590 J/g-°C
    @Temperature 400 °C
    Thermal Conductivity 14.0 W/m-K
    @Temperature 20.0 °C
     16.0 W/m-K
    @Temperature 100 °C
     17.0 W/m-K
    @Temperature 200 °C
     19.0 W/m-K
    @Temperature 300 °C
     20.0 W/m-K
    @Temperature 400 °C
     
    Component Elements PropertiesOriginal ValueComments
    Carbon, C <= 0.030 %
    Chromium, Cr 21.5 - 23 %
    Iron, Fe 63.7 - 70.4 %As Balance
    Manganese, Mn <= 2.0 %
    Molybdenum, Mo 3.0 - 3.5 %
    Nickel, Ni 5.0 - 6.5 %
    Nitrogen, N 0.15 - 0.20 %
    Phosphorus, P <= 0.025 %
    Silicon, Si <= 1.0 %
    Sulfur, S <= 0.015 %

    Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

    Users viewing this material also viewed the following:
    AISI Type 316L Stainless Steel, annealed sheet
    Outokumpu 2205 Duplex Stainless Steel
    AK Steel 2205 Duplex Stainless steel
    Sandvik SAF 2205 Billet
    Sandvik SANMAC SAF 2205 Bar Steel

    NSANDV203 / 19097

    Free Trade Publications, Click Here!
    Free Trade Publications, Click Here!

    Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

    The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.