MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
SEKISUI SPI ALLEN® 6000 PMMA/ABS
Categories: Polymer; Thermoplastic; ABS Polymer; Acrylonitrile Butadiene Styrene (ABS), Sheet

Material Notes: Tri-layered PMMA/ABS Sheet

ALLEN® 6000 is designed for outdoor applications that require protection from UV exposure. It also works well for indoor applications when specialty colors, metallic effects and depth of image are needed. Low gloss matte version available.

ALLEN® 6000 is created with a unique three-layer extrusion process to enable its unique set of properties. And it Underwriters Laboratories, Inc® recognized for UL Std 94 HB (UL94).

Suggested Applications:

  • Agricultural & Heavy Equipment
  • All Terrain/Utility Terrain Vehicles
  • Marine parts
  • Drink Dispensers
  • Recreational Vehicle
  • Sink & Bath

Features:

  • Excellent Weather-ability
  • Superior Smooth Finish (Gloss version)
  • Good Chemical Resistance
  • Abrasion Resistance
  • Low Gloss version
  • Excellent Depth of Image

Information provided by Sekisui Polymer Innovations

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.06 g/ccASTM D792
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 31.0 MPaASTM D638
Tensile Strength, Yield 34.4 MPaASTM D638
Elongation at Break 7.8 %ASTM D638
Elongation at Yield 2.9 %ASTM D638
Tensile Modulus 1999.4 MPaASTM D638
Flexural Strength 68.9 MPaASTM D790
Flexural Modulus 2068.4 MPaASTM D790
Izod Impact, Notched 213 J/m
@Temperature 22.8 °C
ASTM D256
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) 79.4 °CUnannealed; ASTM D648
Flammability, UL94 HB
@Thickness 1.52 mm
Underwriters Laboratories., Inc®; Component Recognition; UL Standard 94
 
Optical PropertiesOriginal ValueComments
Gloss 90 %60° Angle; ASTM D523
 
Descriptive Properties
Motor Vehicle Safety StandardPassesFMVSS 302

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
LyondellBasell Hifax TYC007P BLK Thermoplastic Olefinic Elastomer, mineral Filled
Borealis Daplen™ EE255AE Polypropylene TPO Compound
Borealis Daplen™ EE260AE Scratch Resistant Polypropylene Compound
Ineos Nova 5104 High Impact Polystyrene
Ineos Nova PS9410 High Impact Polystyrene

PSEKIS012 / 185837

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.