MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metal adhesives

(Viewing data as-entered. Click here to return)
Permabond ES562 Epoxy Resin
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy Adhesive

Material Notes: PERMABOND® ES562 is a single-part epoxy adhesive which flows like solder when heated during curing. The adhesive has excellent adhesion to metal surfaces and composites. The high bond strength of this adhesive allows it to replace mechanical fastening, soldering or brazing. The adhesive’s low viscosity is such that it self-levels.

Features & Benefits:

  • Excellent adhesive strength
  • Excellent resistance to vibration
  • Easy to use – no mixing required
  • High shear strength
  • High temperature resistance
  • Good resistance to chemicals

Information provided by Permabond.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.20 g/ccUncured
Viscosity 15000 - 30000 cP
@Temperature 25.0 °C
Uncured
Storage Temperature 2.00 - 7.00 °C
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 80ISO 868
Adhesive Bond Strength 14.0 - 27.0 MPaAluminum, Shear; ISO 4587
 14.0 - 27.0 MPaZinc, Shear; ISO 4587
 20.0 - 35.0 MPaSteel , Shear; ISO 4587
 
Thermal PropertiesOriginal ValueComments
CTE, linear 45.0 µm/m-°C
Thermal Conductivity 0.550 W/m-K
 
Processing PropertiesOriginal ValueComments
Cure Time <= 180 secInduction
 0.500 hour
@Temperature 150 °C
Oven
 0.750 hour
@Temperature 120 °C
Oven
Shelf Life 6.00 Month
 
Descriptive Properties
AppearanceWhiteUncured
Maximum Gap Fill (mm)0.25
Strength Retention100% at 0°CRelative to 0°C
 25% at 200°CRelative to 0°C
 65% at 150°CRelative to 0°C
 85% at 100°CRelative to 0°C
 95% at 50°CRelative to 0°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Epoxy Technology EPO-TEK® H61 Thermally Conductive Epoxy
NuSil EPM-2890 Silicone, Thermal Interface Material (TIM): Adhesive
NuSil CV-2900 Silicone, Thermally Conductive
Permabond ET536 Epoxy Resin
Permabond ET538 Epoxy Resin

PPERMA897 / 162770

Metal adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.