MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
LG Chemical LUTENE® LB7500N Low Density Polyethylene
Categories: Polymer; Thermoplastic; Polyethylene (PE); Low Density (LDPE)

Material Notes: Applications: Flexible package (tie layer or sealant layer of laminating film), Paper and paper board

Typical properties:

  • LUTENE® LB7500N is mainly intended for extrusion coating and can be processed at high speed with uniform thickness and width.
  • LUTENE® LB7500N has a good adhesion strength with Al-foil, polymer film, paper, paper board and other substrate and excellent neck-in characteristics.
  • LUTENE® LB7500N contains no additives.
  • LUTENE® LB7500N complies with U.S. FDA 21CFR 177.1520 C and EU Directive 2002/72 /EC and its amendments and hence Article 3 of European Regulation No. 1935/2004

Information provided by LG Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.918 g/ccASTM D792
Melt Flow 7.8 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
Neck In 2.50 cmat speed 150m/min
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 43ASTM D2240
Tensile Strength at Break 11.3 MPaASTM D638
Tensile Strength, Yield 89.7 kg(f)/cm²ASTM D638
Elongation at Break >= 500 %ASTM D638
 
Thermal PropertiesOriginal ValueComments
Melting Point 106 °C
Vicat Softening Point 83.0 °CASTM D1525
 
Compliance PropertiesOriginal ValueComments
European Food 1935/2004 Yes
FDA Yes
 
Descriptive Properties
Max. Coating Speedat weight 9g/m2
Min. Coating Weightat speed 550m/min

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PLHCHEM9864 / 239380

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.