MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

ZEON Hydrin® PX Epichlorohydrin Elastomer (ECO)
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: Hydrin PX is an adhesion promoter for Hydrin compounds to aid in bonding to FKM, nylon, also other rubber compounds. Hydrin PX was created for use with peroxide cures. Hydrin PX is supplied as a powder.

Hydrin® epichlorohydrin (ECO) elastomers provide an excellent balance of heat (125°C), oil, fuel, and ozone resistance with superior low temperature flexibility. Hydrin is broadly used in automotive fuel hose, air ducts, A/C, and vibration dampening. Its electrical properties benefit laser printer rolls. Hydrin is classified as a CH polymer according to SAE J200 / ASTM D2000.

Information provided by Zeon Chemicals.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 125 °C257 °F
 
Descriptive Properties
MH14-22Test 2084
ML2-6Test 2084
t'20.3-0.8Test 2084
t'903.8 - 6.6Test 2084

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PZEON943 / 250121

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.