MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Mallard Creek Polymers Tylac® 4901 Self Stabilizing Latex
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: Tylac® 4901 self stabilizing latex is a multi-functional styrene-butadiene copolymer additive for down hole cementing applications. Tylac® 4901 is designed for applications providing gas migration coating in cemented annuli, and excellent cement bonding properties while also contributing to exceptional fluid-loss control at low loading levels. Tylac® 4901 also offers consistently good rheology of cement slurries during placement, rapid gel strength upon setting, and turn delivering durability throughout the life of the well. It provides concrete slurry stability over a large range of temperatures, densities and cement systems.

Tylac® 4901 Performance Results: Tylac® 4901 was evaluated and tested by a third party laboratory for properties including: fluid loss, free fluid, rheology properties, thickening time, compressive strength, static gel strength and permeability. Tylac® 4901 performed exceptionally well under all testing categories required for a latex cement system. The following tables and charts illustrate those results.

Featured Benefits:

  • Excellent Control of Gas Migration
  • Good Thermal Stability
  • Improved Wettability for Increased Bonding Strength
  • Flexural Strength Modification
  • Yield Enhancement of Cementitous Slurries
  • Low Viscosity with High Yield Performance
  • Extreme Hydrophilic Stability
  • Fresh and Seawater Stability
  • Excellent Alkali and Acidic Chemical Resistance

Information provided by Mallard Creek Polymers

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Solids Content 47 - 51.5 %
Particle Size 0.24 µm
pH 7.0 - 8.5
Brookfield Viscosity <= 750 cP#20/200
 
Chemical PropertiesOriginal ValueComments
Styrene Content 65 %Bound
 
Descriptive Properties
EmulsifiersAnionic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Polybutadiene Rubber (BR)
Hydrogenated Nitrile Rubber (HNBR)

PMCP125 / 157402

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.