MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
ExxonMobil Mobil Delvac 75W-90 Synthetic Gear Oil
Categories: Fluid; Lubricant

Material Notes: Mobil Delvac Synthetic Gear Oil 75W-90 and 80W-140 are synthetic drivetrain lubricants engineered to meet the most demanding extended drain and warranty requirements. These products are designed for use in heavy-duty drivetrains that require gear lubricants with relatively high viscosity and excellent load-carrying capability and where extreme pressures and shock loading are expected. Mobil Delvac Synthetic Gear Oil 75W-90 and 80W-140 incorporate the latest technology in synthetic basestocks and advanced additives providing significant advantages over mineral gear oils. The technology in Mobil Delvac Synthetic Gear Oil 75W-90 and 80W-140 delivers performance for low and high temperature application, protection against thermal degradation and oxidation, reduced wear and corrosion, improved shear stability, extended service capability, and excellent fuel economy. These products meet API service MT-1/GL-5 EP gear oil service classification and perform at the MIL-PRF-2105E level. The outstanding performance of this product is confirmed by its approval for final drives covered by Eaton Roadranger (E500) and ArvinMeritor Extended Warranties of 750,000 miles, with extended oil drains of 500,000 miles. They are also approved by Mack against GO-J Plus (75W-90) and GO-J (80W-140) extended service classifications.

Heavy-duty manual transmissions, axles and final drives requiring API GL-5 and MT-1 performance; On-highway light and heavy-duty trucks, busses and vans; Off-highway industries including: construction, mining, quarrying, and agriculture; Other heavy-duty industrial gear drives including hypoid and worm gears operating under conditions where high speed/shock load, high speed/low torque, and/or low speed/high torque conditions prevail; Mobil Delvac Synthetic Gear Oil 75W-90 and 80W-140 are intended for initial fill, topping-off or refilling differentials, final drives, transfer cases and other gear applications where lubricants meeting MIL-PRF-2105E, API Service GL-5 , EP gear lubricants are recommended; Recommended for equipment such as winch reduction gears and crawler vehicle propulsion gear drives that are exposed to severe low temperatures; Use as a companion with Mobil Delvac Synthetic Transmission Fluid 50 in transmissions for maximum drive train life, efficiency and fuel economy improvement; Recommended where extended service intervals and warranties are required; Not recommended for applications requiring API GL-4 Level performance; Not intended for automatic, manual or semiautomatic transmissions for which engine oil or automatic transmission fluids are recommended

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.859 g/cc
@Temperature 15.0 °C
ASTM D4052
Viscosity Measurement 140Index; ASTM D2270
Kinematic Viscosity at 40°C (104°F) 120 cStASTM D445
Kinematic Viscosity at 100°C (212°F) 15.9 cStASTM D445
 
Thermal PropertiesOriginal ValueComments
Pour Point -48.0 °CASTM D97
Flash Point 205 °CASTM D92

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
ChevronTexaco TEGRA® SAE 75W-90 Synthetic Gear Lubricant
ChevronTexaco RPM® SAE 75W-90 Synthetic Gear Lubricant
Phillips 66 MP Gear Lube SAE Grade 75W-90

WEXXON053 / 75478

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.