MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Zircar Zirconia ZYW-15 Zirconia Cloth Insulation
Categories: Ceramic; Machinable Ceramic; Oxide; Zirconium Oxide

Material Notes: Zirconia Cloths Type ZYW are flexible textiles composed of yttria stabilized zirconia fibers that offer extreme temperature and chemical resistance in a flexible form. Type ZYW cloths provide the lowest thermal conductivity of any commercially available refractory material in their class. Type ZYW cloths are true textiles, manufactured using the Zircar process where an organic cloth is converted into an inorganic replica. The fabrics are constructed of continuous individual filaments mechanically interlocked in a woven structure.

ZYW ceramic textiles are ideal for temperatures up to 2200°C and are suitable for applications such as high energy battery separators, thermal insulation in crystal growing furnaces, and hot gas filtration. The fine capillary and pore structure of ZYW, in combination with the hydrophilic nature of zirconia, impart excellent wetting, solution retention, and wicking characteristics, to these materials. The cloths require neither binders nor supporting wires to maintain their construction and will comply somewhat to both tensile and compressive forces due to the mechanical interlocking of the fibers. Elongation of 4 to 8% before breaking allows ZYW to conform to irregular surfaces. ZYW can be compressed up to two-thirds of its normal thickness and still recover a major fraction of its original dimension with little fiber damage.

Zirconia Cloth Type ZYW is available in two formats; Type ZYW-15 and Type ZYW-30A. Type ZYW-15 is a square weave cloth nominally 0.015” thick composed of yttria-stabilized zirconia fibers. Type ZYW-30A is a satin weave cloth nominally 0.025” thick.

Features:

  • Low Thermal Conductivity
  • High Porosity
  • Offered in Two Constructions: Square Weave and Satin Weave
  • Extreme High Temperature Stability
  • Fibers Stabilized with ~10 wt% Yttria
  • Can be Cemented with Zircar Zirconia Cement Type ZR-CEM
  • Can be Rigidized with Zircar Zirconia Rigidizer Type ZR-RIG
  • Easily Cut to Size
  • Available ‘off the shelf’

Information provided by Zircar Zirconia.

Key Words: ZrO2, zirconium oxide
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Bulk Density 1.02 g/cc
Porosity 87 %Bulk
Thickness 15.0 mil
Vapor Pressure 8.00e-12 torr
@Temperature 2498 °C
 
Thermal PropertiesOriginal ValueComments
Specific Heat Capacity 0.130 BTU/lb-°F
@Temperature 93.3 °C
 0.180 BTU/lb-°F
@Temperature 2370 °C
Melting Point 2590 °C
Maximum Service Temperature, Air 2200 °CContinuous
Shrinkage 5.5 %
@Temperature 899 °C,
Time 3600 sec
1 hour isothermal soak at 1650°F
 
Component Elements PropertiesOriginal ValueComments
HfO2 1.0 - 2.0 %
Y2O3 10 %
ZrO2 88 - 89 %
 
Descriptive Properties
Tensile Strength per Unit Width154 gram/cm width
Trace Impurities<0.25%
Weight Per Area291 g/m2

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Zircar Zirconia ZYP-30 Zirconia Powder
Zircar Zirconia CeW-30 Ceria Woven Textile Insulation
Zircar Zirconia CeW-15 Ceria Woven Textile Insulation
S-Glass Fiber, Generic
NeoGraf GRAFOIL® GTJ Standard Fluid Sealing Graphite, Single Layer Material

C6ZIR019 / 2775

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.