MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Parker Chomerics Tecknit Consil®-II 842 Molded Silver-Filled Silicone Elastomer
Categories: Polymer; Thermoset; Silicone

Material Notes: Description: CONSIL-II is a molded silicone elastomer filled with silver-coated inert particles. It provides high electrical conductivity, broadband shielding and moisture sealing. CONSIL-II is designed to provide reliable cost effective shielding for a wide range of EMI applications. CONSIL-II is manufactured in sheets, molded parts, strips, and die cut flat gaskets.

Applications: CONSIL-II should be used where there is a need for high broadband shielding combined with excellent moisture sealing properties

Information provided by Chomerics

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.61 - 2.11 g/ccASTM D792
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 60 - 80ASTM D2240
Tensile Strength >= 120 psiASTM D412
Elongation at Break >= 120 %ASTM D412
Tear Strength 45.0 pliASTM D624
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity <= 0.010 ohm-cm
Shielding Effectiveness 75 dB
@Frequency 100000 Hz
H-Field
 90 dB
@Frequency 1e+10 Hz
Plane Wave
 >= 100 dB
@Frequency 1e+9 Hz
Plane Wave
 130 dB
@Frequency 1e+7 Hz
E-Field
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 177 °C
Minimum Service Temperature, Air -51.0 °C
 
Descriptive Properties
BinderSilicone
ColorTan
FillerSilver-plated glass particles

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PCHOME369 / 131079

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.