MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Teknor Apex Vital-Line SHM3905G Flexible Polyvinyl Chloride
Categories: Polymer; Thermoplastic; Vinyl (PVC); PVC, Flexible Grade

Material Notes: Availability: Asia Pacific. Form: granules. Features: Non-phthalate plasticizer, radiation sterilizable. Processing Method: Injection molding. Uses: medical/healthcare applications.

Typical temperature profile for processing compound is from 145°C to 190°C. The optimum temperatures depend on the type of machine as well as screw design being used to process. Feeding zone: 145°C, mold temperature: 0°C-50°C, nozzle zone: 150-170°C, melt temperature: 160°-190°C.

Information provided by Teknor Apex.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.22 - 1.26 g/cc0.0441 - 0.0455 lb/in³ASTM D792
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 84 - 9084 - 90ASTMD2240
Tensile Strength, Yield >= 14.7 MPa>= 2130 psi20 in/min; ASTM D638
Elongation at Break 320 %320 %ASTM D638
 
Descriptive Properties
Heat Stability> 30 min, ASTM D2115-92, 374°F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Armacell Ensolite™ IG2 PVC/NBR/CR
Formosa Plastics Formolon® 690 PVC
Formosa Plastics Formolon® 685 PVC
Formosa Plastics Formolon® 680H PVC
Denka VINYKON R2001 PVC, R grade for hard extrusion

PTEKNN9641 / 231042

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.