MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Raschig Group SURAPLAST UPA 63 UP
Categories: Polymer; Thermoset; Filled/Reinforced Thermoset; Polyester, TS; Thermoset Polyester Glass Filled BMC

Material Notes: Glass fiber reinforced polyester molding compound. Minimal mold shrinkage and post-shrinkage, very good arc resistance, very good mechanical strength. This product meets the allowed upper limits for heavy metals and PCAs and also conforms to the requirements of the EU directives 2002/95 (RoHS), 2002/96 (WEEE) and 2006/122 (PFOS).

Processing: Injection molding

Information provided by the Raschig Group

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.90 - 2.10 g/cc1.90 - 2.10 g/ccISO 1183
Apparent Bulk Density 0.650 - 0.850 g/cc0.0235 - 0.0307 lb/in³ISO 60
Water Absorption <= 0.50 %
@Temperature 23.0 °C,
Time 86400 sec
<= 0.50 %
@Temperature 73.4 °F,
Time 24.0 hour
ISO 62
Linear Mold Shrinkage 0.0010 - 0.0040 cm/cm0.0010 - 0.0040 in/inInjection; ISO 2577
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 50.0 - 70.0 MPa7250 - 10200 psiInjection; ISO 527
Modulus of Elasticity 8.00 - 10.0 GPa1160 - 1450 ksiISO 527
Flexural Strength 140 - 160 MPa20300 - 23200 psiInjection; ISO 178
Flexural Modulus 16.0 - 19.0 GPa2320 - 2760 ksiInjection; ISO 178
Compressive Strength 200 - 250 MPa29000 - 36300 psiISO 604
Charpy Impact Unnotched 1.00 - 1.20 J/cm²
@Temperature 23.0 °C
4.76 - 5.71 ft-lb/in²
@Temperature 73.4 °F
Injection; ISO 179/ 1eU
Charpy Impact, Notched 0.500 - 0.700 J/cm²
@Temperature 23.0 °C
2.38 - 3.33 ft-lb/in²
@Temperature 73.4 °F
Injection; ISO 179/ 1eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+14 - 1.00e+15 ohm-cm1.00e+14 - 1.00e+15 ohm-cmIEC 60093
Surface Resistance 1.00e+13 - 1.00e+14 ohm1.00e+13 - 1.00e+14 ohmIEC 60093
Dielectric Constant  4.0 - 5.0
@Frequency 1e+6 Hz
4.0 - 5.0
@Frequency 1e+6 Hz
IEC 60250
 5.0 - 6.0
@Frequency 100 Hz
5.0 - 6.0
@Frequency 100 Hz
IEC 60250
Dielectric Strength 25.0 - 35.0 kV/mm635 - 889 kV/inIEC 60243-1
Dissipation Factor  0.010 - 0.030
@Frequency 100 Hz
0.010 - 0.030
@Frequency 100 Hz
IEC 60250
 0.010 - 0.030
@Frequency 1e+6 Hz
0.010 - 0.030
@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index 600 V600 VIEC 60112
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 10.0 - 20.0 µm/m-°C
@Temperature 50.0 - 100 °C
5.56 - 11.1 µin/in-°F
@Temperature 122 - 212 °F
ISO 11359-2
Thermal Conductivity 0.900 - 1.10 W/m-K6.25 - 7.63 BTU-in/hr-ft²-°FASTM E1461
Maximum Service Temperature, Air 170 °C338 °F20,000 h; IEC 216/T1
 210 °C410 °F< 50 h; IEC 216/T1
Deflection Temperature at 8.0 MPa >= 200 °C>= 392 °FInjection; ISO 75-C
Flammability, UL94 V-0
@Thickness 0.750 mm
V-0
@Thickness 0.0295 in
Shrinkage <= 0.10 %
@Temperature 110 °C,
Time 605000 sec
<= 0.10 %
@Temperature 230 °F,
Time 168 hour
Post shrinkage; ISO 2577
 
Processing PropertiesMetricEnglishComments
Shelf Life 6.00 Month
@Temperature 15.0 - 25.0 °C
6.00 Month
@Temperature 59.0 - 77.0 °F
 
Descriptive Properties
Arc resistance4 StufeASTM D495
Glow wire ignitability test850/1IEC 60695 2-13
Glow-wire flammability test960/1IEC 60695 2-12
Water Absorption<35 mgISO 62; 24h / 23°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
HK40 CENTRIFUGALLY CAST 25Cr-20Ni-0.4C STEEL TUBES FOR USE IN REFORMER FURNACES (SCH 22-CF)
Cast Stainless Steel HK40, ASTM A351M
Cast Stainless Steel HK40, ACI
Quantum Composites LYTEX® 4084 63% Glass Fiber Reinforced Epoxy SMC
MetalTek MTEK HK40 Cast UNS J94204 Heat Resistant Stainless Steel

PRASCH22 / 65307

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.