MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Renishaw 8045-2 Polyurethane Resin
Categories: Polymer; Thermoset; Polyurethane, TS

Material Notes: Description: Translucent PP/PE type

Features: Variable hardness, pigmentable

Suitable for: High Impact, snap fit applications

Information provided by Renishaw

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.16 g/cc1.16 g/ccCured
Viscosity Measurement 220220[Mpa], Cured
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 6161
Tensile Strength 12.0 MPa1740 psiISO 527
Elongation at Break 65 %65 %ISO 527
Tensile Modulus 0.400 GPa58.0 ksiISO 527
Flexural Strength 11.0 MPa1600 psiISO 178
Flexural Modulus 0.300 GPa43.5 ksiISO 178
Izod Impact, Notched (ISO) 19.0 kJ/m²9.04 ft-lb/in²ISO 180
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 42.0 °C108 °FISO 75-1
 
Processing PropertiesMetricEnglishComments
Cure Time 60.0 min
@Temperature 60.0 °C
1.00 hour
@Temperature 140 °F
Pot Life 5.00 min
@Load 0.100 kg
5.00 min
@Load 0.221 lb
 
Descriptive Properties
ColorTransparentCured
Mixing ratio by weight100:140:50
Molding colorTranslucent

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PRENISH003 / 206366

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.