MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Tra-Con Tra-Bond Ablebond 933-1.5 Moisture Resistant Encapsulant
Categories: Polymer; Thermoset; Epoxy; Filled/Reinforced Thermoset

Material Notes: TRA-BOND 933-1.5 electrically insulating epoxy encapsulant is formulated to provide a smooth crown over the device of wire bonds. This encapsulant provides protection from thermal and mechanical shock. The long work life and smooth consistency of TRA-BOND 933-1.5 encapsulant make it ideal for use in automatic dispensers. This compound is stable at room temperature for up to three (3) months; however since the filler may settle, we recommend storage at -40°C or colder.

Information provided by Tra-Con Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.50 g/cc1.50 g/ccMixed
Viscosity 10000 cP10000 cPMixed
 
Chemical PropertiesMetricEnglishComments
Ionic Impurities - Na (Sodium) 15 ppm15 ppm
Ionic Impurities - K (Potassium) 1.0 ppm1.0 ppm
Ionic Impurities - Cl (Chloride) 380 ppm380 ppm
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 9090
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 5.30e+14 ohm-cm5.30e+14 ohm-cm
Dielectric Constant 3.83.8
Dielectric Strength 59.1 kV/mm1500 kV/in
Dissipation Factor 0.00700.0070
 
Thermal PropertiesMetricEnglishComments
CTE, linear 47.0 µm/m-°C26.1 µin/in-°FBelow Tg
 150 µm/m-°C83.3 µin/in-°FAbove Tg
Thermal Conductivity 0.400 W/m-K
@Temperature 121 °C
2.78 BTU-in/hr-ft²-°F
@Temperature 250 °F
Glass Transition Temp, Tg 109 °C228 °FUltimate Tg
 
Processing PropertiesMetricEnglishComments
Cure Time  30.0 min
@Temperature 150 °C
0.500 hour
@Temperature 302 °F
 120 min
@Temperature 125 °C
2.00 hour
@Temperature 257 °F
Working Life 130000 min
@Temperature 25.0 °C
130000 min
@Temperature 77.0 °F
Shelf Life 12.0 Month
@Temperature -40.0 °C
12.0 Month
@Temperature -40.0 °F
 
Descriptive Properties
Color Black
Weight Loss % 1.7At 300°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Tra-Con Tra-Bond 972-1 Thermally Conductive Flexible Epoxy Adhesive
Tra-Con Tra-Bond 789-4 Thermally Conductive Adhesive
Tra-Con Tra-Bond Ablebond 862-2 Room Temperature Cure Epoxy Adhesive
Tra-Con Tra-Bond Ablebond 744-2NTN1 Electrically Insulating Polyimide Adhesive
Tra-Con Tra-Bond 968-5 High Dielectric Constant Epoxy Adhesive

PTRAC203 / 71131

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.