MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Colmant Coated Fabrics Natural Rubber Coated Cotton Fabric
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Cotton is a natural fiber of vegetable origin. The cotton thread is derived from the transformation of Gossypium bristles (or cotton). Commonly we also referred under the same name the fabric after the weaving of the wire. Cotton is the first textile fiber used in the world despite the advent of synthetic fibers. It is inflammable and starts decomposition at 160 ° C. Cotton is popular thanks to its characteristics: aspect, lightness, comfort and ease of assembly and processing. Natural rubber is to be considered as the sole non-synthetic rubber. This particular rubber can be recycled for the reutilization, mostly for the manufacturing of tires. New methods of recycling natural rubber are under development to diminish the ecological impact of used tires and other products. Detaining excellent physical properties (elongation at break, tensile strength and abrasion) and presented in a widespread range of hardness, natural rubber has the best elasticity among all rubbers. Under ambient conditions (a mix of the right temperature, sun exposition, rain and wind) natural rubbers shows almost perfect fatigue resistance, excellent compression and tear strength which makes it ideal for any dynamic applications.

Applications:

  • Industrial fabrics
  • straps
  • tarps
  • tires
  • rope
  • clothing
  • Automobile door seals
  • hoses
  • profiles for windows and doors
  • tennis or golf balls, gloves
  • tubes and pipes
  • tires
  • coated fabrics
  • roofing
  • pharmaceutical stoppers
  • seals
  • tires
Properties:
  • Fireproofed
  • Abrasion resistance
  • Non-skid

Information provided by COLMANT COATED FABRICS

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 30 - 9030 - 90
Tensile Strength at Break 8.00 - 20.0 MPa1160 - 2900 psi
Elongation at Break 100 - 900 %100 - 900 %
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 70.0 °C158 °F
Minimum Service Temperature, Air -50.0 °C-58.0 °F
 
Descriptive Properties
IRHD Hardness30-90
Point Temperature-50 C° - 80°C
Warp breaking strength75 - 120 daN/5cm
Warp elongation at break10% - 20%
Weft breaking strength70 - 90 daN/5cm
Weft elongation at break10% - 20%
Weight per sqm200 - 400

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PCOLMANT078 / 316128

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.