MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

CHT HANSA CARE 1050 Silicone polymer
Categories: Other Engineering Material

Material Notes: Description: This kind of silicone polymer is ideal to reduce the surface tension of liquid formulation to ensure a good spreading and wetting during application.

Key Features

  • Wetting effect
  • Leveling effect
  • Cleansing effect
  • Sheeting effect
Key Applications
  • Floor Care
  • Leather Care
  • Furniture Care
  • Car Care
Application: Due to the non-ionic character of HANSA CARE 1050 it can be easily combined with other finishing products. Its low surface tension enables an easy wetting of polar and non-polar hydrophobic surfaces such as e.g. polyethylene, polyvinyl chloride or siliconised materials by aqueous systems. This will improve the adhesion of care films, adhesives or coatings.

Addition Rates
Dosage – 1: 0.1 - 0.5% in total formulations for leveling
Dosage – 2: 2.0 - 5.0% in rinse aid formulations for commercial vehicles

Information provided by CHT Group

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.00 - 1.04 g/cc0.0361 - 0.0376 lb/in³BS ISO 2781
Volatiles 0.00 %0.00 %
Brookfield Viscosity <= 100 cP<= 100 cP
Storage Temperature 4.00 - 40.0 °C39.2 - 104 °F
 
Processing PropertiesMetricEnglishComments
Shelf Life 24.0 Month24.0 Month
 
Descriptive Properties
AppearanceColorless to yellow liquid
ChemistryPolyether modified polysiloxane
IonicityNon-ionic
MIT FreeYes
Ultralow cyclic contentYes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PCHTSIL350 / 314833

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.