MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Spartech SP-3010 Rigid PVC Specialty Sheet
Categories: Polymer; Thermoplastic; Vinyl (PVC); PVC, Sheet Grade

Material Notes: Description: Specialty Sheet

Information provided by Spartech.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.40 g/ccASTM D792
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 112ASTM D785
Tensile Strength, Yield 6600 psiASTM D638
Tensile Modulus 400000 psiASTM D638
Flexural Yield Strength 12000 psiASTM D790
Flexural Modulus 480000 psiASTM D790
Izod Impact, Unnotched 14.0 ft-lb/inASTM D256
 0.500 ft-lb/in
@Temperature -40.0 °C
ASTM D256
Falling Dart Impact 31.0 ft-lb73°F; ASTM D3029
 8.00 ft-lb
@Temperature -40.0 °C
ASTM D3029
 
Thermal PropertiesOriginal ValueComments
CTE, linear 40.0 µin/in-°F
@Temperature 20.0 °C
ASTM D696
Deflection Temperature at 1.8 MPa (264 psi) 155 °FASTM D648
Flammability, UL94 V-0
 
Optical PropertiesOriginal ValueComments
Gloss 90 %Gardner; ASTM D2523

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Kostat ICP-STAT ICS-1004 PVC Sheet
Overview of materials for PVC, Sheet Grade
Geon® Performance Solutions Vinyl Rigid Extrusion L6181 Polyvinyl Chloride, Rigid
Geon® Performance Solutions Vinyl Packaging VEO-184 Polyvinyl Chloride, Rigid
Geon® Performance Solutions Vinyl Packaging PK8-1080 Polyvinyl Chloride, Rigid

PSPAR064 / 68505

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.