MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Plastics Group Polifil® BS-7010 70% Barium Sulfate Reinforced Polypropylene
Categories: Polymer; Thermoplastic; Polypropylene (PP)

Material Notes: Polifil® BS series compounds are homopolymer polypropylene resins reinforced with barium sulfate. They possess increased specific gravity, high flex modulus, high deflection temperature, good chemical resistance, frictional resistance, and x-ray opacity. These compounds are utilized in cosmetic application, molded weights, soundproofing components, and medical devices. Standard processing techniques are applicable.

Information provided by The Plastics Group.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 2.03 g/cc2.03 g/ccASTM D792
Filler Content 70.0 %70.0 %TPG WI
Water Absorption 0.000 %
@Time 86400 sec
0.000 %
@Time 24.0 hour
ASTM D570
Linear Mold Shrinkage 0.00600 cm/cm0.00600 in/in0.098" wall
Melt Flow 10.0 g/10 min
@Load 2.16 kg,
Temperature 230 °C
10.0 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 15.2 MPa2200 psiASTM D638
Elongation at Break 20.0 %20.0 %ASTM D638
Flexural Strength 20.7 MPa3000 psiASTM D790
Flexural Modulus, 1% Secant 1930 MPa280000 psiASTM D790
Izod Impact, Notched 0.214 J/cm0.400 ft-lb/inASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 124 °C255 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 65.6 °C150 °FASTM D648

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PPOLI107 / 325320

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.