MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Akrochem RESINALL® 1030 Resin
Categories: Polymer; Thermoplastic

Material Notes: Product Description: Resinall 1030 hydrogenated cycloaliphatic hydrocarbon resin based on the thermal polymerization of dicyclopentadiene mixtures. It contains no aromaticity. This resin has very low color, low odor, and excellent thermal stability. It tackifies ethylene vinyl acetate (EVA), styrene block copolymers (SIS, SBS, SEBS), metallocene polyethylene, and amorphous poly-alpha olefins (APAO). This balance of properties makes it ideally suited for use in rubber based adhesives for packaging.

Information provided by Akrochem Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.08 g/cc
 
Thermal PropertiesOriginal ValueComments
Melting Point 130 °CBall & Ring
 
Optical PropertiesOriginal ValueComments
Gardner Color Number <= 1.0100% solid
 
Descriptive Properties
Appearanceflake

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PAKZCH384 / 315302

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.