MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Solder Replacement
RoHS Compliant Adhesives for Solder Replacement
Master Bond offers RoHS compliant, electrically conductive systems to replace lead soldering. These epoxy and silicone adhesives offer low volume resistivity, low outgassing and high temperature resistance.

Superior Flux Superior No. 141 Soft Soldering Flux
Categories: Metal; Nonferrous Metal; Solder/Braze Alloy

Material Notes:
  • Non-Hazardous, water-based flux.
  • Complies with ASTM and CDA specifications.
  • Formulated for lead-free alloys.
Description: Superior No. 141 plumbing flux is a creamy, white, water flushable paste that holds its shape and will not slump until being heated above 50°C/122°F. This product was developed as a water-flushable alternative to petroleum-based plumbing fluxes, the current standard. Superior No. 141 meets ASTM Specification B-813 and complies with Copper Development Association (CDA) requirements. It is a water-based flux that promotes excellent solderability and post-solder removal with lead-free solders.

Applications: Superior No. 141 is formulated specifically for use in plumbing applications where Copper and Copper-alloy tubes are being soldered. It is also an excellent choice for Copper pipes used in heating, air-conditioning, mechanical, and fire sprinkler systems.

Information provided by Superior Flux

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.990 g/cc0.990 g/cc
Density 0.985 g/cc0.0356 lb/in³
pH 0.00 - 2.00.00 - 2.0
Viscosity 117000 cP117000 cP
 
Thermal PropertiesMetricEnglishComments
Melting Point -10.0 °C14.0 °FFreezing Point
 60.0 °C140 °F
 
Processing PropertiesMetricEnglishComments
Processing Temperature 93.0 - 315 °C199 - 599 °FSoldering Range
Shelf Life 2.00 Month2.00 Month
 
Descriptive Properties
ColorWhite
FormPaste
ResiduesWater Flushable

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

NSFLUX046 / 185730

solder replacement adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.