MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Taiwan PU Corporation TPL-THANE 5085-A/B High Pressure Urethane Spraying Elastomer
Categories: Polymer; Thermoset; Polyurethane, TS; Rubber or Thermoset Elastomer (TSE)

Material Notes: 5085-A is a high reactivity polyethamine content extender. 5085-B is a methylene diphenyklene dissocyanate(MDI). They make up the third generation high pressure urethane spraying elastomer. It has excellent physical properties, chemical resistance, and abrasion resistance.

Applications:

  • Protective coating
  • Abrasion resistant coating
  • Pipe coating
  • Flooring
  • Roof and deck coating
  • Construction coating
  • Industrial coating
  • Low cost molds
  • Spray-mold type
  • Highway and bridge overlays
  • Watertight coating
  • Roller, other casting elastomer replacement
  • Foam surface protection

Information provided by Taiwan PU Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.01 g/cc0.0365 lb/in³A component
 1.10 g/cc0.0397 lb/in³B component
Viscosity 500 - 700 cP500 - 700 cPA component
 1000 - 1200 cP1000 - 1200 cPB component
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 85 - 9085 - 90
Tensile Strength at Break >= 7.85 MPa>= 1140 psi
Elongation at Break >= 300 %>= 300 %
Tear Strength >= 29.4 kN/m>= 168 pli
 
Processing PropertiesMetricEnglishComments
Processing Temperature 60.0 - 65.0 °C140 - 149 °FTemperature setting, B component
 65.0 - 70.0 °C149 - 158 °FTemperature setting, A component
 
Descriptive Properties
Mixing Ratio1:1

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PTPU60 / 70916

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.