Features and Typical Applications: Provide excellent heat dissipation and thermal shock resistance as well as protection from moisture and chemical agents. Typical applications include sensors, transformers, transducers, switches, and other small devices.
Emerson & Cuming 1495/11 Stycast® Two-Component Thermally Conductive Encapsulant
- Mix Ratio by weight = 100:5
- Good Chemical Resistance
- Filled
- High temperature
Cure Type: Heat Bonding Type: Epoxy The Stycast® product line is now a part of Henkel; this specific grade is discontinued. |