MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Momentive Performance Materials RTV159 High Strength Silicone Adhesive Sealant, Red
Categories: Polymer; Adhesive; Thermoset; Silicone; Silicone, RTV, Adhesive/Sealant Grade

Material Notes: RTV 159 is a one component, ready-to-use, high strength silicone rubber adhesive sealant. It cures to tough resilient silicone rubber on exposure to atmospheric moisture at room temperature. RTV159 sealant also provides high temperature performance. It releases acetic acid vapors as a by-products of cure.

RTV159 sealant is a paste consistency product which can be applied to horizontal, vertical, and overhead surfaces in applications requiring high strength and temperature performance.

Since this adhesive sealants utilizes a moisture cure system, it must not be used in thicknesses greater than 6mm(1/4in.). Where section depths exceed 6mm (1/4 in.), GE Silicones one-component, addition cure or two-component silicone rubber compounds are suggested.

This sealant was not designed for and should not be used for applications intended for permanent implantation into the human body.

Mechanical properties for specimen cured 3 days at 25°C and 50% relative humidity.

Key Performance Properties:

  • High strength
  • High temperature performance
  • Low temperature flexibility
  • One-component
  • Room temperature cure
  • General primerless adhesion
  • Excellent electrical insulation properties
  • Excellent weatherability, ozone, and chemical resistance

GE Silicones became a part of Momentive Performance Materials in 2006.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.09 g/cc
Linear Mold Shrinkage 0.010 cm/cm
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 28
Tensile Strength, Ultimate 72.1 kg(f)/cm²Cured 7 days at 25°C and 50% relative humidity
Elongation at Break 825 %
Tear Strength 16.1 kg(f)/cm
Peel Strength 60.0 pliCured 7 days at 25°C and 50% relative humidity
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.10e+15 ohm-cm
Dielectric Constant 2.6
Dielectric Strength 19.7 kV/mm
Dissipation Factor 0.00070
 
Thermal PropertiesOriginal ValueComments
CTE, linear 270 µm/m-°C
@Temperature 20.0 °C
Thermal Conductivity 0.000500 cal cm/sec-cm²-°C
Maximum Service Temperature, Air 260 °CContinuous
 315 °CIntermittent
Brittleness Temperature -60.0 °C
 
Processing PropertiesOriginal ValueComments
Tack-Free Time 0.750 hour
 
Descriptive Properties
Application rate175 g/min
ColorRed
ConsistencyPaste

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Momentive Performance Materials RTV162 Electronic Grade Silicone Adhesive Sealant, White
Momentive Performance Materials RTV160 Electronic Grade Silicone Adhesive Sealant, White
Momentive Performance Materials RTV157 High Strength Silicone Adhesive Sealant, Gray
Dow Silastic® 9416/50 KIT PARTS A&B
Precision Polymer Engineering S50D Silicone Rubber

PGESIL022 / 41013

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.