MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Proto3000 – 3D Engineering Solutions

Kraiburg TPE THERMOLAST® K TF8AAB Thermoplastic Elastomer (FC/HE/tl Series) Adhesion to PP
Categories: Polymer; Thermoplastic; Elastomer, TPE; Styrenic TPE

Material Notes: The FC/HE/tl series is a material solution for everyday life applications with regulatory requirements. The series is characterized by its high elastic properties and its adhesion to PP. The translucent materials can be colored in many different ways.

Processing Method: Injection Molding, Extrusion

Color / RAL DESIGN:

  • Translucent
Typical applications:
  • Household articles
  • Flexible Connections
  • Membranes
  • Seals for housings
  • Valves
  • Packaging (for food and care products)
  • Closures
  • Toys
Material advantages:
  • Hysteresis
  • Colorable
  • Optimized mechanical properties
  • In-process recycling possible
  • High elasticity
  • Adhesion to PP
  • Free from animal ingredients

Information provided by Kraiburg TPE

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.890 g/cc0.0322 lb/in³DIN EN ISO 1183-1
Storage Temperature 15.0 - 30.0 °C59.0 - 86.0 °F
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 7575DIN ISO 48-4
Tensile Strength 17.5 MPa2540 psi200 mm/min; DIN 53504/ISO 37
Elongation at Break 750 %750 %200 mm/min; DIN 53504/ISO 37
Tear Strength 27.0 kN/m154 pliISO 34-1 Method B (b)
Compression Set  30 %
@Temperature 23.0 °C,
Time 259000 sec
30 %
@Temperature 73.4 °F,
Time 72.0 hour
DIN ISO 815-1 Method A
 47 %
@Temperature 70.0 °C,
Time 86400 sec
47 %
@Temperature 158 °F,
Time 24.0 hour
DIN ISO 815-1 Method A
 66 %
@Temperature 100 °C,
Time 86400 sec
66 %
@Temperature 212 °F,
Time 24.0 hour
DIN ISO 815-1 Method A
 
Descriptive Properties
ColorTranslucent

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PKRAIA8209 / 308873

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.