MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Akrochem Accelerator TETD
Categories: Other Engineering Material

Material Notes: Product Description: Accelerator TETD is a very active, sulfur-bearing, non-discoloring rubber accelerator for use in natural and synthetic rubber systems. It can be used alone or combination with many other common rubber accelerators.

Application: TETD functions as a primary accelerator for cure systems requiring very low or no sulfur. It is cure modifier in W/G-type neoprenes. It is often used in conjunction with thiazole or sulfenamide curing systems. Accelerator TETD contains 10.8% available sulfur. Normally zinc oxide and a fatty acid are required when using TETD in a natural rubber application. Sulfur is not required, but is often used. TETD can be blended with TMTD to reduce the tendency of the compound to bloom while maintaining cure activity. Accelerator TETD is also available as Akroform® TETD-75. This polymeric masterbatch contains 75% Accelerator TETD. Polymer bound or encapsulated dispersions are a proven means of upgrading plant safety, efficiency, quality & raw material control.

Information provided by Akrochem Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.30 g/cc
Ash <= 0.30 %
 
Thermal PropertiesOriginal ValueComments
Melting Point 69.0 - 73.0 °C
 
Processing PropertiesOriginal ValueComments
Moisture Content <= 0.30 %
 
Descriptive Properties
Appearancebuff to light gray granules

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PAKZCH457 / 315375

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.