MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Eastman Tritan™ Renew EX501-50 Copolyester
Categories: Polymer; Thermoplastic; Polyester, TP

Material Notes: Eastman Tritan™ Renew EX501-50 is an amorphous copolyester specifically developed for the Infant Care market. Its most outstanding features are consistent glass-like clarity even after multiple dishwasher cycles. Additionally, Tritan Renew EX501-50 exhibits low taste and odor retention versus cPP, excellent drop impact resistance, and dishwasher durability. Tritan Renew EX501-50 contains a mold release derived from vegetable based sources. Tritan Renew EX501-50 meets infant care sterilization requirements via boiling water or microwave steam sterilization. This new-generation copolyester can also be molded into various applications without incorporating high levels of residual stress. Combined with Tritan's outstanding chemical resistance and hydrolytic stability, these features give molded products enhanced durability in the dishwasher environment, which can expose products to high heat, humidity, and aggressive cleaning agents. Tritan Renew EX501-50 can be converted into parts using injection molding, injection stretch blow molding (ISBM), and extrusion blow molding techniques. Tritan Renew EX501-50 copolyester may be used in repeated-use food contact articles under United States Food and Drug Administration (FDA) regulations. Contact an Eastman representative for details on global food contact regulatory clearances. Tritan Renew EX501-50 copolyester is included in Eastman Chemical Company’s Customer Notification Procedure which details our policy for customer notification when significant changes are made in Tritan™ Renew EX501-50 sold into the infant care market. This procedure provides the infant care industry an added layer of confidence in the consistent quality and performance of Tritan™. Eastman Renew polymers have been certified by International Sustainability & Carbon Certification (ISCC), a global, independent agency for tracking sustainable content in a variety of industries. Renew polymers are produced with ISCC certified circular content by mass balance allocation.

Applications

  • Baby bottles/sippy cups
  • Childcare items
Key Attributes
  • Dishwasher durability: Chemical resistance; Heat resistance; Hydrolytic stability
  • Drop impact resistance
  • Glass-like clarity
  • Global food contact regulatory clearances
  • Low taste and odor retention
  • Stain resistance
  • Sterilization capable via microwave steaming and boiling water immersion

Information provided by Eastman.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.18 g/cc0.0426 lb/in³ASTM D792
Linear Mold Shrinkage 0.00500 - 0.00700 cm/cm0.00500 - 0.00700 in/inASTM D955
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 109109ASTM D785
Tensile Strength at Break 55.0 MPa7980 psiISO 527
 56.0 MPa8120 psiASTM D638
Tensile Strength, Yield 44.0 MPa6380 psiISO 527
 45.0 MPa6530 psiASTM D638
Elongation at Break 151 %151 %ISO 527
 176 %176 %ASTM D638
Elongation at Yield 6.00 %6.00 %ISO 527
 6.00 %6.00 %ASTM D638
Tensile Modulus 1.516 GPa219.9 ksiASTM D638
 1.538 GPa223.1 ksiISO 527
Flexural Yield Strength 72.0 MPa10400 psiASTM D790
Izod Impact, Notched  0.720 J/cm
@Temperature -40.0 °C
1.35 ft-lb/in
@Temperature -40.0 °F
ASTM D256
 10.24 J/cm
@Temperature 23.0 °C
19.18 ft-lb/in
@Temperature 73.4 °F
ASTM D256
Izod Impact, Unnotched  NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
ASTM D4812
 NB
@Temperature -40.0 °C
NB
@Temperature -40.0 °F
ASTM D4812
Izod Impact, Notched (ISO)  14.0 kJ/m²
@Temperature -40.0 °C
6.66 ft-lb/in²
@Temperature -40.0 °F
ISO 180
 114 kJ/m²
@Temperature 23.0 °C
54.2 ft-lb/in²
@Temperature 73.4 °F
ISO 180
Puncture Energy  57.0 J
@Temperature 23.0 °C
42.0 ft-lb
@Temperature 73.4 °F
ASTM D3763
 66.0 J
@Temperature -40.0 °C
48.7 ft-lb
@Temperature -40.0 °F
ASTM D3763
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 101 °C214 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 88.0 °C190 °FASTM D648
 
Optical PropertiesMetricEnglishComments
Haze <= 1.00 %<= 1.00 %ASTM D1003
 6.00 %6.00 %After 8 hr boiling
Transmission, Visible 91.0 %91.0 %Total; ASTM D1003
 
Processing PropertiesMetricEnglishComments
Processing Temperature 80.0 - 90.0 °C176 - 194 °FBlow Mold Temperature
 185 - 195 °C365 - 383 °FPreform Temperature at Blow
Melt Temperature 260 - 282 °C500 - 540 °FInjection Molding
 270 - 285 °C518 - 545 °FInjection Stretch Blow Molding
Mold Temperature 38.0 - 66.0 °C100 - 151 °FInjection Molding
 60.0 - 70.0 °C140 - 158 °FInjection Stretch Blow Molding
Drying Temperature 88.0 °C190 °FTypical
Dry Time 4.00 - 6.00 hour4.00 - 6.00 hourTypical
Dew Point <= -35.0 °C<= -31.0 °FTypical
 
Compliance PropertiesMetricEnglishComments
FDA YesYesSee notes for details
 
Descriptive Properties
Blow Pressure0.03-0.08 MPaPrimary
 0.2-0.3 MPaSecondary

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PEATM4204 / 323827

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.