MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Overview of materials for Nylon 66, Heat Stabilized
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, Heat Stabilized

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Heat Stabilized". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 1.04 - 2.50 g/ccAverage value: 1.31 g/cc Grade Count:819
Filler Content 13.0 - 60.0 %Average value: 34.1 % Grade Count:56
Water Absorption 0.0100 - 8.90 %Average value: 1.45 % Grade Count:457
Moisture Absorption at Equilibrium 0.250 - 2.90 %Average value: 2.02 % Grade Count:100
 1.00 - 3.40 %
@Temperature 70.0 - 70.0 °C
Average value: 1.95 % Grade Count:38
Water Absorption at Saturation 2.50 - 10.0 %Average value: 5.58 % Grade Count:113
Viscosity 18.0 - 70000 cP
@Temperature 100 - 2000 °C
Average value: 8480 cP Grade Count:9
 18.0 - 70000 cP
@Shear Rate 60.0 - 10000 1/s
Average value: 8480 cP Grade Count:9
Viscosity Number 130 - 150 cm³/gAverage value: 145 cm³/g Grade Count:6
Maximum Moisture Content 0.0200 - 0.200Average value: 0.150 Grade Count:71
Linear Mold Shrinkage 0.000100 - 0.0335 cm/cmAverage value: 0.00811 cm/cm Grade Count:597
 0.00400 - 0.0200 cm/cm
@Temperature 80.0 - 80.0 °C
Average value: 0.0146 cm/cm Grade Count:22
Linear Mold Shrinkage, Transverse 0.00100 - 0.0980 cm/cmAverage value: 0.00988 cm/cm Grade Count:194
 0.00800 - 0.0200 cm/cm
@Temperature 80.0 - 80.0 °C
Average value: 0.0156 cm/cm Grade Count:22
Melt Flow 1.00 - 50.0 g/10 minAverage value: 9.72 g/10 min Grade Count:27
Spiral Flow 0.800 - 115 cmAverage value: 81.3 cm Grade Count:20
Ash 0.800 - 58.0 %Average value: 25.1 % Grade Count:18
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 55.0 - 119Average value: 78.4 Grade Count:32
Hardness, Rockwell R 82.0 - 125Average value: 114 Grade Count:194
Ball Indentation Hardness 130 - 370 MPaAverage value: 274 MPa Grade Count:52
Tensile Strength, Ultimate 8.00 - 1020 MPaAverage value: 126 MPa Grade Count:527
 40.0 - 150 MPa
@Temperature 60.0 - 150 °C
Average value: 98.1 MPa Grade Count:7
 50.0 - 175 MPa
@Temperature 60.0 - 140 °C
Average value: 98.1 MPa Grade Count:2
 50.0 - 175 MPa
@Strain 0.750 - 6.00 %
Average value: 98.1 MPa Grade Count:2
Tensile Strength, Yield 10.3 - 248 MPaAverage value: 108 MPa Grade Count:322
 144.79 - 144.79 MPa
@Temperature 93.3 - 93.3 °C
Average value: 145 MPa Grade Count:1
Elongation at Break 1.00 - 300 %Average value: 20.1 % Grade Count:740
 3.20 - 80.0 %
@Temperature 60.0 - 150 °C
Average value: 69.4 % Grade Count:6
Elongation at Yield 2.00 - 90.0 %Average value: 16.0 % Grade Count:97
Modulus of Elasticity 0.0848 - 31.0 GPaAverage value: 8.63 GPa Grade Count:299
 0.400 - 9.20 GPa
@Temperature 60.0 - 150 °C
Average value: 2.28 GPa Grade Count:5
Flexural Yield Strength 18.0 - 420 MPaAverage value: 165 MPa Grade Count:631
 35.0 - 35.0 MPa
@Temperature 90.0 - 90.0 °C
Average value: 35.0 MPa Grade Count:1
Flexural Modulus 0.255 - 61.4 GPaAverage value: 6.10 GPa Grade Count:673
 0.750 - 15.1685 GPa
@Temperature 90.0 - 93.3 °C
Average value: 7.96 GPa Grade Count:2
Flexural Strain at Break 3.00 - 7.50 %Average value: 4.60 % Grade Count:5
Compressive Yield Strength 30.3 - 110 MPaAverage value: 57.0 MPa Grade Count:3
Poissons Ratio 0.300 - 0.400Average value: 0.347 Grade Count:7
Shear Strength 50.0 - 76.5 MPaAverage value: 61.7 MPa Grade Count:5
Secant Modulus 2.00 - 17.5 GPa
@Temperature 60.0 - 140 °C
Average value: 5.42 GPa Grade Count:2
 2.00 - 17.5 GPa
@Strain 0.000 - 8.00 %
Average value: 5.42 GPa Grade Count:2
Izod Impact, Notched 0.320 - 13.2 J/cmAverage value: 1.70 J/cm Grade Count:353
 1.0678 - 2.40255 J/cm
@Temperature -40.0 - -30.0 °C
Average value: 1.31 J/cm Grade Count:5
 0.5339 - 2.6695 J/cm
@Temperature -40.0 - -40.0 °C
Average value: 1.31 J/cm Grade Count:16
 0.5339 - 2.6695 J/cm
@Thickness 3.17 - 3.17 mm
Average value: 1.31 J/cm Grade Count:16
Izod Impact, Unnotched 0.0816 - 5340 J/cmAverage value: 8.23 J/cm Grade Count:82
 0.900 - 0.900 J/cm
@Temperature -30.0 - -30.0 °C
Average value: 0.900 J/cm Grade Count:1
Izod Impact, Notched (ISO) 1.57 kJ/m² - NBAverage value: 21.6 kJ/m² Grade Count:273
 3.00 - 17.0 kJ/m²
@Temperature -40.0 - -30.0 °C
Average value: 8.44 kJ/m² Grade Count:30
Izod Impact, Unnotched (ISO) 30.0 - 21000 kJ/m²Average value: 64.7 kJ/m² Grade Count:40
 25.0 - 90.0 kJ/m²
@Temperature -30.0 - -30.0 °C
Average value: 62.7 kJ/m² Grade Count:12
Charpy Impact Unnotched 1.30 J/cm² - NBAverage value: 8.12 J/cm² Grade Count:251
 0.000 J/cm² - NB
@Temperature -40.0 - -20.0 °C
Average value: 6.83 J/cm² Grade Count:118
Charpy Impact, Notched 0.280 - 2100 J/cm²Average value: 1.71 J/cm² Grade Count:409
 0.200 J/cm² - NB
@Temperature -40.0 - -20.0 °C
Average value: 1.17 J/cm² Grade Count:118
Coefficient of Friction 0.100 - 0.280Average value: 0.225 Grade Count:11
Coefficient of Friction, Static 0.0900 - 0.220Average value: 0.170 Grade Count:11
K (wear) Factor 16.1 - 38.3 x 10-8 mm³/N-MAverage value: 31.3 x 10-8 mm³/N-M Grade Count:11
Limiting Pressure Velocity 0.596 - 1.54 MPa-m/secAverage value: 0.690 MPa-m/sec Grade Count:8
Taber Abrasion, mg/1000 Cycles 4.00 - 7.00Average value: 6.11 Grade Count:9
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 1.00 - 2.44e+17 ohm-cmAverage value: 2.76e+15 ohm-cm Grade Count:358
Surface Resistance 1.00 - 1.00e+16 ohmAverage value: 1.86e+14 ohm Grade Count:186
Insulation Resistance 100000 - 1.00e+12 ohmAverage value: 3.33e+11 ohm Grade Count:3
Dielectric Constant 2.70 - 13.0Average value: 4.07 Grade Count:59
Dielectric Strength 9.84 - 120 kV/mmAverage value: 25.9 kV/mm Grade Count:287
Dissipation Factor 0.00900 - 0.320Average value: 0.0610 Grade Count:46
Arc Resistance 95.0 - 185 secAverage value: 127 sec Grade Count:6
Comparative Tracking Index 225 - 650 VAverage value: 517 V Grade Count:124
 
Thermal PropertiesOriginal ValueComments
CTE, linear 7.20 - 146 µm/m-°CAverage value: 44.5 µm/m-°C Grade Count:236
 102 - 102 µm/m-°C
@Temperature 35.0 - 55.0 °C
Average value: 102 µm/m-°C Grade Count:1
 102 - 102 µm/m-°C
@Thickness 2.00 - 2.00 mm
Average value: 102 µm/m-°C Grade Count:1
CTE, linear, Transverse to Flow 22.0 - 124 µm/m-°CAverage value: 68.8 µm/m-°C Grade Count:37
Specific Heat Capacity 1.67 J/g-°CAverage value: 1.67 J/g-°C Grade Count:7
Thermal Conductivity 0.200 - 0.260 W/m-KAverage value: 0.218 W/m-K Grade Count:11
Melting Point 220 - 268 °CAverage value: 259 °C Grade Count:303
Maximum Service Temperature, Air 65.0 - 230 °CAverage value: 150 °C Grade Count:45
Deflection Temperature at 0.46 MPa (66 psi) 100 - 263 °CAverage value: 236 °C Grade Count:398
Deflection Temperature at 1.8 MPa (264 psi) 50.0 - 262 °CAverage value: 187 °C Grade Count:589
Deflection Temperature at 8.0 MPa 80.0 - 235 °CAverage value: 203 °C Grade Count:29
Vicat Softening Point 150 - 255 °CAverage value: 243 °C Grade Count:72
Glass Transition Temp, Tg 5.00 - 72.0 °CAverage value: 38.5 °C Grade Count:7
UL RTI, Electrical 65.0 - 110 °CAverage value: 81.4 °C Grade Count:3
UL RTI, Mechanical with Impact 65.0 - 110 °CAverage value: 81.4 °C Grade Count:3
UL RTI, Mechanical without Impact 65.0 - 110 °CAverage value: 84.3 °C Grade Count:3
Flammability, UL94 HB - 5VAGrade Count:367
Flame Spread 0.000 - 100 mm/minAverage value: 8.33 mm/min Grade Count:12
Oxygen Index 21.0 - 34.0 %Average value: 25.4 % Grade Count:34
Glow Wire Test 649 - 960 °CAverage value: 777 °C Grade Count:76
 
Processing PropertiesOriginal ValueComments
Processing Temperature 260 - 310 °CAverage value: 281 °C Grade Count:79
Nozzle Temperature 240 - 310 °CAverage value: 281 °C Grade Count:58
Melt Temperature 225 - 330 °CAverage value: 281 °C Grade Count:255
Mold Temperature 21.1 - 150 °CAverage value: 83.3 °C Grade Count:310
Drying Temperature 65.6 - 120 °CAverage value: 81.0 °C Grade Count:266
Moisture Content 0.0300 - 0.250 %Average value: 0.168 % Grade Count:124
Dew Point -17.8 °CAverage value: -17.8 °C Grade Count:7
Injection Pressure 4.96 - 138 MPaAverage value: 48.5 MPa Grade Count:48
Vent Depth 0.000762 - 0.00127 cmAverage value: 0.00109 cm Grade Count:11

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Nylon 66, Unreinforced
Overview of materials for Nylon 66, Impact Grade
Overview of materials for Nylon 66, 10% Glass Fiber Filled
Overview of materials for Nylon 66/6
Overview of materials for Nylon 66, 30% Glass Fiber Filled

O2504 / 78003

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.