MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Copper, UNS C41500, H02 Temper flat products
Categories: Metal; Nonferrous Metal; Copper Alloy

Material Notes: Good to excellent corrosion resistance. Excellent cold workability, good hot formability. Fabricated by blanking, drawing, bending, forming, shearing and stamping.

Applications: spring applications for electrical switches.

Test specimen: flat products - 1mm thickness.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.80 g/cc0.318 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell B 7474
Hardness, Rockwell 30T 6565
Tensile Strength, Ultimate 385 MPa55800 psi
Tensile Strength, Yield  365 MPa
@Strain 0.5 %
52900 psi
@Strain 0.5 %
 370 MPa
@Strain 0.2 %
53700 psi
@Strain 0.2 %
Elongation at Break 16 %16 %In 50 mm
Modulus of Elasticity 110 GPa16000 ksiHard
 125 GPa18100 ksiAnnealed
Poissons Ratio 0.280.28Calculated
Machinability 30 %30 %UNS C36000 (free-cutting brass) = 100%
Shear Modulus 46.0 GPa6670 ksi
Shear Strength 280 MPa40600 psi
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00000620 ohm-cm
@Temperature 20.0 °C
0.00000620 ohm-cm
@Temperature 68.0 °F
 
Thermal PropertiesMetricEnglishComments
CTE, linear 18.6 µm/m-°C
@Temperature 20.0 - 300 °C
10.3 µin/in-°F
@Temperature 68.0 - 572 °F
Specific Heat Capacity 0.380 J/g-°C0.0908 BTU/lb-°F
Thermal Conductivity 123 W/m-K
@Temperature 20.0 °C
854 BTU-in/hr-ft²-°F
@Temperature 68.0 °F
Melting Point 1010 - 1032 °C1850 - 1890 °F
Solidus 1010 °C1850 °F
Liquidus 1032 °C1890 °F
 
Processing PropertiesMetricEnglishComments
Annealing Temperature 400 - 705 °C752 - 1300 °F
Hot-Working Temperature 730 - 845 °C1350 - 1550 °F
 
Component Elements PropertiesMetricEnglishComments
Copper, Cu 89 - 93 %89 - 93 %
Iron, Fe <= 0.050 %<= 0.050 %
Lead, Pb <= 0.10 %<= 0.10 %
Tin, Sn 1.5 - 2.2 %1.5 - 2.2 %
Zinc, Zn 7.2 %7.2 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

MC41500b6 / 11298

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.